SGCC Prepainted thiab Kub Dip Galvanized Steel Chev
Galvanized steel phaj yog los tiv thaiv nto los ntawm corrosion thiab ncua lub neej kev pab cuam ntawm steel nto, coated nrog ib txheej ntawm hlau .zinc tus huab tais ntawm zinc coated nyias phaj hu ua galvanized ntawv..
Kub-dip galvanized yog kub - dov steel coils, los yog txias-kuav los tiag steel raws li ib tug substrate, tom qab ib tug tas mus li kub-dip galvanized txheej txheem thiab ces tsim. Qhov hla mus rau ib daim duab plaub uas rau cov khoom siv yog kub dip galvanized ntawv; los ntawm kev nqa-up txhawm rau muab cov khoom kub yob galvanized ntim. Yog li ntawd, kub-dip galvanizing tuaj yeem muab faib ua cov kub dov galvanized coils thiab txias dov coils, uas feem ntau yog siv hauv kev tsim kho, tsev tuav khoom, tsheb, thawv, thauj thiab tsev neeg ua lag luam thiab lwm yam kev lag luam, tshwj xeeb tshaj yog, steel siv, tsheb tsim, steel silo manufacturing thiab lwm yam lag luam.
Specifications
Thickness: {{0}}.13mm TCT txog 4.0mm TCT.
Dav: 600mm txog 1250mm.
Zinc Txheej: 40-275G/M2.
Chromated, Qhuav, daim tawv nqaij-dhau, Tshav theem, ci ntsa iab. Oiled los yog Unoiled.
Tsis tu ncua Spangle, yam tsawg kawg nkaus Spangle, Loj Spangle, Zero Spangle.
Temper: Full Hard (85-95 HRB; G550). Kev Lag Luam Zoo (50-75 HRB; G350).
Coil Luj: 3-6 MT.
Coil ID: 508mm lossis 610mm.
Kev Xa Khoom: Los ntawm Tej lossis Los ntawm 20GP Thawv.
Waterproof Standard Export Packing.
Cov nqe lus them nqi: los ntawm T / T lossis L / C ntawm Pom.
Delivery: 15 Hnub.
|
STEEL Qib |
CHEMICAL |
MECHANIC |
CB OB |
Txheej |
||||||
|
C |
Si |
Mn |
S |
P |
T.S |
Y.S |
E.L |
|||
|
x103 |
x103 |
x102 |
x103 |
x103 |
Mpa |
Mpa |
% |
d =0 180 degree |
G/M² |
|
|
JIS G3302 SGCC |
12 |
30 |
41 |
31 |
21 |
480 |
300 |
13 |
OK |
Z60-150 |
|
JIS G3302 SGCH |
12 |
10 |
21 |
18 |
8 |
680 |
650 |
OK |
Z60-150 |
|
|
ASTM A653 CS.B |
20 |
30 |
60 |
35 |
30 |
386 |
205~380 |
20 |
OK |
Z80-275 |
|
DX51D+Z |
29 |
21 |
18 |
1.8 |
11 |
355 |
245 |
38 |
OK |
Z80-275 |
|
G550 |
20 |
6 |
73 |
5 |
17 |
715 |
654 |
8 |
OK |
Z80-275 |

FAQ
1.Q: Koj puas yog lub Hoobkas lossis tuam txhab lag luam?
A: Peb yog cov chaw tsim khoom, thiab peb lub tuam txhab kuj yog ib lub tuam txhab kev lag luam rau cov khoom siv steel.Peb tuaj yeem muab ntau yam khoom siv hlau.
2.Q: Koj lub Hoobkas ua li cas txog kev tswj xyuas zoo?
A: Peb tau txais ISO, CE thiab lwm yam ntawv pov thawj. Los ntawm cov ntaub ntawv mus rau cov khoom, peb xyuas txhua tus txheej txheem kom tswj tau qhov zoo.
3.Q: Kuv puas tuaj yeem tau txais cov qauv ua ntej xaj?
A: Yog lawm, tau kawg. Feem ntau peb cov qauv yog dawb. peb tuaj yeem tsim los ntawm koj cov qauv lossis cov duab kos duab.
4.Q: Koj ua li cas rau peb lub lag luam mus ntev thiab kev sib raug zoo?
A: Peb khaws cov khoom zoo thiab cov nqi sib tw kom ntseeg tau tias peb cov neeg siv khoom tau txais txiaj ntsig; Peb hwm txhua tus neeg siv khoom raws li peb tus phooj ywg thiab peb ua siab dawb ua lag luam thiab ua phooj ywg nrog lawv. Txawm lawv tuaj qhov twg los.
5.Q: Koj lub sijhawm xa khoom yog dab tsi?
A: Peb lub sijhawm xa khoom yog li ib lub lis piam, lub sijhawm raws li cov neeg siv khoom.
Cim npe nrov: Prepainted galvanized steel sgcc, Tuam Tshoj prepainted galvanized steel sgcc manufacturers, lwm tus neeg, Hoobkas