Dab tsi yog qhov txawv ntawm Galvanized Steel Chev DX53D thiab DX54D?

Dec 29, 2025

Galvanized Steel Chev

 

DX53D Galvanized Steel Chev yog kub dip galvanized steel khoom tsim raws li EN 10346 tus qauv. Nws muaj kev sib sib zog nqus kos duab zoo heev, cov khoom siv kho tshuab ruaj khov, thiab muaj zog tiv thaiv corrosion los ntawm cov xim zinc txheej. Lub ntsej muag spangle tsis tu ncua muab qhov zoo nkauj hlau ua tiav thaum tuav cov txheej txheem txhim khu kev qha.

 

DX53D Galvanized Steel Chev yog siv dav hauv cov qauv tsheb, cov khoom siv hauv tsev, HVAC systems, thiab cov vaj huam sib luag tsim, tshwj xeeb tshaj yog nyob rau hauv cov ntawv thov uas yuav tsum muaj ob qho tib si tsim muaj peev xwm thiab ntev - lub sij hawm durability.

 

Galvanized Steel Coil

Technical Specifications ntawm DX53D Galvanized Steel Chev

 

Parameter Tus nqi
Txuj TS EN 10346
Qib xwm 53d
Thickness 0.30-3.00 hli
Dav 600-1500 hli
Zinc Txheej Z100 – Z275 g/m²
Spangle Hom Tsis tu ncua
Kev kho saum npoo Chromated / Passivated / Oiled
Formability Zoo heev
Weldability Zoo

 

Mechanical Properties

 

Khoom Tus nqi
Yield zog 140-220 MPa
Tensile zog 270-350 MPa
Elongation Ntau dua lossis sib npaug li 36%
Khoov Performance Zoo heev
Deep Drawing Performance Superior

 

DX54D yog qhov zoo tshaj plaws kos duab- qib zoo hauv EN 10346 DX series. Nws muaj qhov siab elongation thiab siab tshaj plaws ductility rau cov kev ua haujlwm nyuaj tshaj plaws.

 

DX54D Cov ntsiab lus tseem ceeb

 

Parameter Tus nqi
Txuj TS EN 10346
Qib xwm 54d
Elongation Ntau dua lossis sib npaug li 40%
Formability Zoo heev
Daim ntawv thov Automotive txheej panels, complex lub cev qhov chaw

 

DX53D vs DX54D: Hauv -Kev sib piv qhov tob

 

Feature xwm 53d xwm 54d
Elongation Ntau dua lossis sib npaug li 36% Ntau dua lossis sib npaug li 40%
Daim duab sib sib zog nqus Zoo heev Zoo heev
Nto Stability Zoo heev Zoo heev
Txheej Adhesion Zoo heev Zoo heev
Nqi Efficiency Siab Nruab nrab
Kev tsim khoom nyuaj Tsawg Nruab nrab
Tej kev siv Cov khoom siv, cov khoom siv plhaub Automotive sab nrauv panels

 

Manufacturing Case Analysis

Ib lub chaw tsim khoom tsheb tsim cov khoom sib sib zog nqus- tsim lub qhov rooj ntsuas ob qho tib si DX53D Regular Spangle Galvanized Steel Coil thiab DX54D. Tom qab kev sim, DX53D tau raug xaiv rau cov khoom siv sab hauv, thaum DX54D tau tshwj tseg rau cov vaj huam sib luag pom sab nrauv uas xav tau kev tsim kho huab cua. Kev sib xyaw ua ke kom zoo txo ​​cov khoom siv tag nrho los ntawm 11% yam tsis muaj kev cuam tshuam cov khoom zoo.

 

Txawm hais tias DX54D muaj qhov zoo tshaj plaws ductility, DX53D Regular Spangle Galvanized Steel Chev muab qhov zoo sib npaug ntawm formability, lub zog, nqi efficiency, thiab ntau lawm stability. Nws txhawb nqa cov txheej txheem sib sib zog nqus nrog cov cuab yeej qis dua thiab zoo heev ntawm qhov sib xws.

Qhov no ua rau DX53D yog qhov kev xaiv pheej yig tshaj plaws rau siab - ntim khoom lag luam.

 

Lub zinc txheej ntawm DX53D Regular Spangle Galvanized Steel Coil ua ob qho tib si tiv thaiv thiab kev txi anode. Txawm tias nyob rau hauv marine los yog industrial cheeb tsam, lub txheej tseem ceeb ncua kev xeb tsim, ua kom lub neej ntev kev pab cuam thiab txo nqi txij nkawm.

 

Kev lag luam kev siv

 

Cov kev lag luam tseem ceeb uas siv DX53D Regular Spangle Galvanized Steel Chev suav nrog:

  • Automotive kev tsim khoom
  • Kev tsim khoom siv
  • Kev tsim kho lag luam
  • Infrastructure thiab kev thauj mus los
  • Zog thiab cua tshuab

Kev nce thoob ntiaj teb kev thov rau cov khoom siv ruaj khov thiab hnyav txuas ntxiv nthuav dav DX53D kev siv thoob ntiaj teb.

 

GNEE STEEL muab cov khoom siv siab- zoo DX53D Galvanized Steel Chev nrog kev tswj xyuas nruj, kev sib tw nqi, thiab kev lag luam thoob ntiaj teb txhim khu kev qha. Txhua kauj yog tsim raws li cov qauv thoob ntiaj teb thiab kho kom haum raws li cov neeg siv khoom tshwj xeeb.

 

Nrog xyoo dhau los ntawm kev xa tawm, GNEE STEEL txhawb nqa cov neeg siv khoom thoob plaws ntau qhov kev lag luam nrog kev ua haujlwm zoo, kev pabcuam tshaj lij, thiab kev txawj ntse.

 

Hu rau GNEE STEEL hnub no kom tau txais cov lus sib tw thiab kev sib tham txog kev tshaj lij.

 

Hu rau tam sim no

 

  • Mechanical Properties

 

Qib Txheej Txuj Yield zog Re (MPa) Tensile zog Rm (MPa) Elongation A80 (min %) r90 (min) n90 (min)
xwm 51d Z, ZA, ZF TS EN 10346 - 270 – 500 22 - -
xwm 52d Z, ZA, ZF TS EN 10346 140 – 300 ²) 270 – 420 26 - -
xwm 53d Z, ZA, ZF TS EN 10346 140 – 260 270 – 380 30 - -
xwm 54d Z, ZA, ZF TS EN 10346 120 – 220 260 – 350 36 1.6 ⁴) 0.18
xwm 56d Z, ZA, ZF TS EN 10346 120 – 180 260 – 350 39 1.9 ⁵) 0.21 ⁵)
xwm 57d Z, ZA TS EN 10346 120 – 170 260 – 350 41 2.1 ⁵) 0.22