DX53D Regular Spangle Galvanized Steel Coil Siv Corrosion Resistant

Dec 29, 2025

Galvanized hlau

 

DX53D Regular Spangle Galvanized Steel Chev yog lub siab - zoo kub dip galvanized steel khoom tsim raws li EN 10346 tus qauv. Nws yog tsim los rau kev sib sib zog nqus nqus thiab tsim daim ntaub ntawv thaum muab kev tiv thaiv corrosion zoo heev los ntawm zinc txheej. Lub npe "DX" qhia tau hais tias txias- ua steel, "53" sawv cev rau nws cov formability, thiab "D" yog hais txog kev kos duab zoo. Lub spangle nto li niaj zaus yog tsim ib txwm thaum lub sij hawm zinc solidification, muab ob qho tib si kev ua haujlwm corrosion thiab ib qho zoo nkauj hlau zoo nkauj.

 

Vim nws cov khoom ruaj khov, cov txheej txheem zoo dua, thiab qhov ua tau zoo ntawm qhov chaw, DX53D Regular Spangle Galvanized Steel Coil tau dhau los ua ib qho ntawm cov khoom siv nrov tshaj plaws hauv cov khoom siv tsheb, cov khoom siv hauv tsev, vaj huam sib luag, thiab kev lag luam kev lag luam. Nws ua ke ntawm formability thiab corrosion kuj ua rau nws yog ib qho zoo tagnrho tov rau manufacturers nrhiav ob qho tib si kev ua tau zoo thiab kev pab lub neej ntev.

Galvanized Steel Coil

Cov Lus Qhia Tseem Ceeb ntawm DX53D Galvanized Steel Chev

 

Khoom Tus nqi
Txuj TS EN 10346
Qib Steel xwm 53d
Txheej hom Kub Dip Galvanized
Spangle Hom Tsis tu ncua Spangle
Thickness Ntau 0.30-3.00 hli
Dav Ntau 600-1500 hli
Zinc Txheej Z100 – Z275 g/m²
Kev kho saum npoo Passivated, Oiled, Qhuav
Formability Zoo heev
Weldability Zoo

 

Mechanical Performance Overview

 

Parameter Tus nqi
Yield zog 140-220 MPa
Tensile zog 270-350 MPa
Elongation Ntau dua lossis sib npaug li 36%
Khoov Performance Zoo heev
Kev kos duab Superior

Cov khoom no xyuas kom meej tias DX53D Regular Spangle Galvanized Steel Coil ua tau zoo nyob rau hauv cov txheej txheem sib sau ua ke thaum tuav ntev - lub sij hawm corrosion kuj.

 

DX53D vs DX51D: Ib qho piv txwv piv txwv

 

Ntau tus neeg yuav khoom xav txog DX51D ua lwm txoj hauv kev, tab sis rau kev sib sib zog nqus daim ntawv thov DX53D muaj cov txiaj ntsig tseem ceeb.

Feature xwm 51d xwm 53d
Formability Txuj kev tsim Sib sib zog nqus nqus muaj peev xwm
Elongation Ntau dua lossis sib npaug li 22% Ntau dua lossis sib npaug li 36%
Nto Stability Zoo Zoo heev
Kev kos duab zoo Nruab nrab Superior
Kev siv yam Roofing, ncej Automotive qhov chaw, cov khoom siv plhaub

 

Hauv kev tsim khoom, hloov los ntawm DX51D mus rau DX53D galvanized steel coil txo cov kab nrib pleb los ntawm ntau dua 40% thaum cov txheej txheem stamping thaum txhim kho qhov sib xws tom qab tsim.

 

Daim ntawv thov ntawm DX53D Galvanized Steel Chev

 

DX53D Regular Spangle Galvanized Steel Coil yog siv dav hauv:

Automotive lub cev panels thiab qhov cuab lub zog

Cov khoom siv hauv tsev thiab cov khoom siv hauv tsev

Steel qhov rooj, ru tsev panels, thiab phab ntsa cladding

Qhov cua ducts thiab HVAC systems

Hluav taws xob enclosures thiab industrial cov khoom

Nws lub siab elongation thiab txheej adhesion ua kom zoo ib yam nrog cov khoom siv tsawg tsawg.

 

  • Mechanical Properties

 

Qib Txheej Txuj Yield zog Re (MPa) Tensile zog Rm (MPa) Elongation A80 (min %) r90 (min) n90 (min)
xwm 51d Z, ZA, ZF TS EN 10346 - 270 – 500 22 - -
xwm 52d Z, ZA, ZF TS EN 10346 140 – 300 ²) 270 – 420 26 - -
xwm 53d Z, ZA, ZF TS EN 10346 140 – 260 270 – 380 30 - -
xwm 54d Z, ZA, ZF TS EN 10346 120 – 220 260 – 350 36 1.6 ⁴) 0.18
xwm 56d Z, ZA, ZF TS EN 10346 120 – 180 260 – 350 39 1.9 ⁵) 0.21 ⁵)
xwm 57d Z, ZA TS EN 10346 120 – 170 260 – 350 41 2.1 ⁵) 0.22

 

Xaiv GNEE STEEL txhais tau tias ua haujlwm nrog tus neeg muag khoom ntseeg siab uas nkag siab txog kev lag luam steel thoob ntiaj teb thiab muab kev pabcuam kev tshaj lij los ntawm kev nug txog kev xa khoom. Txawm hais tias koj qhov project cuam tshuam nrog kev tsim tsheb, kev tsim kho, lossis kev tsim khoom lag luam, GNEE STEEL ua kom txhua lub kauj ua tau raws li koj qhov kev xav tau thiab kev ua tau zoo.

 

Hu rau GNEE STEEL hnub no kom tau txais koj cov lus hais thiab kev sib tham.

 