SGC440 Kub Dip Galvanized Steel

Khoom: Nruam kub-dip zinc coated Txias dov steels kauj, sawb, phaj, phaj rau kev siv qib: SGC440SGC440 steel zoo: siab zog rau kev siv dav dav SGC440 steel txheej tiav: R (ib txwm spangle), Z (tsawg spangle) SGC440 steel kauj / strip / daim ntawv nto zoo: A (raws li coated nto), B (kho qhov chaw), C (zoo tshaj plaws nto)

Khoom Taw qhia

Khoom Taw qhia

 

SGC440 Hot Dip Galvanized Steel coils

SGC440 Hot Dip Galvanized Steel

SGC440 steel Chev / sawb / daim ntawv kho mob:
C (Chromate kev kho mob), NC (Non Chromate kev kho mob), O (oiling), X (unoiling) NP (phosphating kev kho mob ntawm non chromate), P (Phosphated), M (Untreated)

SGC440 steel kauj / sawb / ntawv txheej loj:
Ntshiab Zinc txheej: Z06 (60g), Z08 (80g), Z10 (100g), Z12 (120g), Z14 (140g), Z18 (180g), Z20 (200g), Z22 (220g), Z25 (250g), Z27 (270g), Z35 (350g), Z37 (370g), Z45 (450g), Z60 (450g)
Alloy Zinc + Fe: F04(40g), F06(60g), F08(80g), F10(10g0), F12(120g), F18(180g)

SGC440 steel kauj / sawb / ntawv txheej: Z (Ntshiab Zinc), ZF (Z + Fe alloy)
JIS G 3302 SGC440 steel haum loj: Thickness 0.25mm-3.2mm

SGC440 steel chemical muaj pes tsawg leeg:

Qib C max Mn max P max S max
SIB 440 0.25 2.0 0.20 0.05


SGC440 steel hlau Mechanical zog

Qib Yield zog MPa Tensile zog MPa Elongation % min
{{0}} 25- Tsawg dua los yog sib npaug li 0.40mm {{0}} 40- Tsawg dua los yog sib npaug li 0.60mm {{0}} 60- Tsawg dua los yog sib npaug li 1.0mm 1.0- Tsawg dua los yog sib npaug li 1.6mm 1.6- Tsawg dua los yog sib npaug li 2.5mm Tshaj 2.5mm
SIB 440 335 nqi 440 min 18 18 18 18 18 18


GNEE STEEL muaj ntau tshaj 2000 tons SGC440 steel Tshuag qhov chaw txhua lub hlis. Peb tuaj yeem ua tau raws li peb cov neeg siv khoom feem ntau ntawm qhov ntau thiab kev thov. Raws li cov khoom lag luam no, peb qhov kev lag luam zoo tshaj plaws kis mus rau cov txheej txheem steel xws li: txiav (ntawm qhov dav thiab ntev), kos duab, rov ntim dua, thiab lwm yam.

SGC440 Hot Dip Galvanized Steel sheet

Cim npe nrov: sgc440 kub dip galvanized steel, Tuam Tshoj sgc440 kub dip galvanized steel manufacturers, lwm tus neeg, Hoobkas