JAC270E Cold Rolled Kub Dip Galvanized Steel

JAC270E steel mob: Chev, sawb, sheetJAC270E steel hlau Nto: Kub dip galvanized (ZF), Oiled (O), BNA, FD / FC / FB, R, DJAC270E steel Main daim ntawv thov: tsheb manufacturing.JAC270E steel haum loj: Thickness 0.4mm-3.2mm

Khoom Taw qhia

Khoom Taw qhia

 

JAC270E txias dov kub-dip galvanized steel yog lub zog siab galvanized sheet coil nrog ntau yam kev siv, feem ntau yog siv hauv kev tsim tsheb, steel qauv vaj tse, khoom siv hauv tsev tsim, ntim khoom, tsheb thauj mus los thiab lwm yam haujlwm. cov
JAC270E txias dov kub-dip galvanized steel yog ib daim hlau nyias nrog ib txheej ntawm zinc adhered rau nws nto los ntawm immersing lub nyias steel ntawv nyob rau hauv ib tug molten zinc da dej.
Lub xeev saum npoo ntawm JAC270E txias dov kub-dip galvanized steel nws txawv nyob ntawm txoj kev kho mob, nrog rau cov zinc spangles zoo tib yam, zoo zinc spangles, tiaj zinc spangles, tsis muaj zinc spangles, thiab phosphating nto. Tsis tas li ntawd, cov ntawv galvanized yuav tsum muaj qhov zoo nkauj thiab yuav tsum tsis txhob muaj qhov tsis zoo uas tsim kev puas tsuaj rau kev siv cov khoom, xws li tsis muaj plating, qhov, tawg, scum, ntau plating thickness, khawb, chromic acid av, xeb dawb, lwm.

 

Txheej khoom Zn-Fe (ZF)
Txheej hom Zn-Fe (ZF) ob-sided txheej 60 ~ 440G / m2, ib sab txheej 30 ~ 220g / m2

 

JAC270E steel Mechanical zog

Qib T (mm) Plasticity nruab nrab
Ua nruj
Yield zog MPa Tensile zog MPa Elongation A80 min
0.5-
1.0
>1.0
-1.6
JAC 270 E 0.4-3.2 Ntau dua lossis sib npaug rau 1.4 Ntau dua lossis sib npaug rau 1.3 110-205 Ntau dua lossis sib npaug li 270 41-55

GNEE STEEL muaj ntau tshaj 2000 tons JAC270E steel Tshuag qhov chaw txhua lub hlis. Peb tuaj yeem ua tau raws li peb cov neeg siv khoom feem ntau ntawm qhov ntau thiab kev thov. Raws li cov khoom lag luam no, peb qhov kev lag luam zoo tshaj plaws kis mus rau cov txheej txheem steel xws li: txiav (ntawm qhov dav thiab ntev), kos duab, rov ntim dua, thiab lwm yam.

JAC270E Cold Rolled Hot Dip Galvanized Steel

Cim npe nrov: jac270e txias dov kub dip galvanized steel, Tuam Tshoj jac270e txias dov kub dip galvanized steel manufacturers, lwm tus neeg, Hoobkas