Zinc Sheet galvanized hlau

Kub Dipped Galvanized Steel Sheet yog tsim los ntawm kev dhau daim ntawv Tag Nrho Hard uas tau ua tiav cov txheej txheem ntxuav cov kua qaub thiab cov txheej txheem dov los ntawm zinc lauj kaub, yog li thov zinc zaj duab xis rau saum npoo. Nws muaj kev tiv thaiv corrosion zoo heev, pleev xim, thiab ua haujlwm tau zoo vim Zinc tus yam ntxwv.

Khoom Taw qhia

Khoom Taw qhia

 

Zinc Sheet galvanized hlau:

Kub Dipped Galvanized Steel Sheet (GI) yog tsim los ntawm kev dhau daim ntawv Tag Nrho Hard uas tau ua tiav cov txheej txheem ntxuav cov kua qaub thiab dov txheej txheem los ntawm lub lauj kaub zinc, yog li thov zinc zaj duab xis rau saum npoo. Nws muaj kev tiv thaiv corrosion zoo heev, pleev xim, thiab ua haujlwm tau zoo vim Zinc tus yam ntxwv.

Galvanized steel ntawv piav qhia:

Dav

500 ~ 1500mm los yog raws li koj qhov kev thov

Thickness

{{0}}.12 ~ 3.0mm los yog raws li koj thov

Ntev

1000mm-12000mm lossis raws li koj qhov kev thov

Ua siab ntev

Thickness & Dav: +/{1}}.02mm

Zinc txheej

40-275g/m2

Cov txheej txheem

Rolled txias los yog kub dov

Txuj

GB / ASTM / JIS / AISI

Qib

Q195,Q235,Q235B,Q345,Q345B

SGCC, DX51D/DX52D, SGCC, DX51D+Z/DX52D+Z

S280GD+Z, S350GD+Z

SGCH, JIS G3302, ASTM A653

Ntim

Nyob rau hauv pob nrog steel sawb los yog ntim rau hauv ntoo pallets los yog raws li cov neeg muas zaub 'yuav tsum tau.

Daim ntawv thov

Muaj vaj huam sib luag, vov tsev, Siding rau painting, Tsev, Phab ntsa, Sab nrauv decorating cov ntaub ntawv thiab lwm yam.

 

 

FAQ

1. Q: Koj puas yog cov chaw tsim khoom lossis tuam txhab lag luam?
A: Peb yog cov chaw tsim khoom nrog 1.5 lab tons ntawm cov hlau txhua xyoo hauv Suav teb. Peb tau dhau lub Hoobkas tshuaj xyuas los ntawm ntau lub koom haum thoob ntiaj teb thiab muaj peb tus kheej pab neeg muag khoom. Txais tos kom pom thiab tshuaj xyuas peb lub Hoobkas
2. Q: Koj puas muaj kev tswj xyuas zoo?
A: Yog, peb muaj iso, bv, sgs certifications thiab peb tus kheej zoo contorl kuaj.
3. Q: Koj lub sijhawm xa khoom ntev npaum li cas?
A: Tsis pub dhau 7-15 hnub tom qab tau txais qhov tso nyiaj lossis L/C thaum pom. Lub sij hawm ua hmoov txhuas ntev yuav xav tau rau cov khoom tsim tshwj xeeb.
4. Q: Koj puas muab cov qauv? puas yog dawb los yog ntxiv?
A: Yog lawm, peb tuaj yeem muab cov qauv dawb tab sis tus nqi xa khoom yuav raug them los ntawm peb cov neeg siv khoom.
5. Q: Koj puas muab kev pabcuam tomqab muag?
A: Peb muab kev pab cuam tom qab muag thiab muab 100% lav rau peb cov khoom ..

 

product-15-15Zinc Sheet galvanized Steel

Cim npe nrov: Zinc Sheet galvanized Steel, Tuam Tshoj Zinc Sheet galvanized Steel manufacturers, lwm tus neeg, Hoobkas

Xa kev nug

Xa kev nug