Tsev-Cov khoom- Galvanized hlau - Galvanized Steel Chev-

Ntsiab lus

video

DC01 Galvanized Steel Chev

galvanized txheej ntawm galvanized steel coil tsim ib qho kev thaiv uas tiv thaiv cov dej noo thiab lwm yam corrosive los ntawm kev nkag mus rau hauv cov hlau, ua rau cov hlau galvanized tiv taus thiab xeb- cov khoom siv tiv taus uas tuaj yeem siv ntau yam kev siv.

Khoom Taw qhia

Khoom Taw qhia

 

DC01 Galvanized Steel Chev

 

DC01 Galvanized Steel Coil

GNEE STEELyog cov chaw tsim khoom thiab cov khoom lag luam ntawm siab - zoo galvanized steel coils. Peb cov khoom suav nrog DC01 galvanized steel coils, daim hlau, kav, PPGI thiab lwm yam khoom siv hlau. DC01 galvanized steel coils yog tsim rau cov khoom siv hauv tsev, kev tsim tsheb, kev kho kom zoo nkauj hauv tsev, cov hlab ntsha siab, cov khoom siv tshuaj, elevator, tsheb thauj mus los, kev tsim khoom, thiab lwm yam.

Txuj: EN 10130, EN 10346

Qib: DC01, Q195, SGCD1, thiab lwm yam.

Tshuab: Txias Rolling, Kub-dip Galvanizing, Electro-galvanizing

Ntawv pov thawj: ISO 9001, CE

Qhov ntev

 

Khoom npe DC01 galvanized steel kauj
Substrate DC01 Txias- dov steel
Thickness 0.15mm-4mm, Customized
Dav 600mm - 2000mm, Customized
Coil puab 508mm - 610mm, Customized
Zinc Txheej 30g – 275g/m²
Spangle loj, tsis tu ncua, mini, thiab xoom spangles
Kev kho saum npoo anti- ntiv tes luam / daim tawv nqaij dhau / oiled / qhuav / chromated / Embossed / Lamination
Txoj Kev Xeem Zinc Txheej Thickness Test, Khoov, Hla-hatch, Tshuaj tsuag ntsev, Tensile Test, thiab lwm yam.
Ua siab ntev ±1%
Kev Pabcuam Bending, Vuam, Decoiling, Txiav, Punching
Invoicing los ntawm qhov hnyav
Lub sij hawm xa tuaj 7-15 hnub
Kev them nyiaj T / T, L / C, Credit Card

 

Tshuaj muaj pes tsawg leeg

 

Element Cov pa roj carbon (C) Manganese (Mn) Phosphorus (P) Sulfur (S) Silicon (Si) Nto zoo
             
Cov ntsiab lus (Max, %) 0.12 0.6 0.045 0.045 0.03 A, B

 

Ntim thiab shipping

 

Cov khoom raug muag zoo hauv tsev thiab txawv teb chaws, thiab raug xa tawm mus rau cov teb chaws xws li Middle East, South America, Europe, thiab Southeast Asia.

Peb siv ntau hom kev ntim khoom rau ntau hom hlau kom ruaj khov, sib khi, thiab tiv thaiv- kho corrosion; tsis tu ncua tshuaj xyuas thiab tswj cov khoom siv thauj mus los kom tsis txhob muaj dej sib xyaw thiab qhov chaw ntub dej; Nyob rau tib lub sijhawm, kos cov ncauj lus kom ntxaws raws li cov qauv thoob ntiaj teb kom muaj kev nyab xeeb thiab zoo ntawm kev thauj mus los steel.

 

DC01 Galvanized Steel Coil

 

GNEE STEEL cov kev tsim nyog

 

DC01 Galvanized Steel Coil

 

GNEE STEEL koom nrog hauv kev nthuav qhia

 

DC01 Galvanized Steel Coil

 

Cim npe nrov: dc01 galvanized steel kauj, Tuam Tshoj dc01 galvanized steel kauj manufacturers, lwm tus neeg, Hoobkas

Xa kev nug

Xa kev nug