DX51D Galvanized Steel Strips 0.8 * 16mm 19mm 25mm 32mm Qhuav Rollal Hlau Galvanized Steel Pluaj Banding

DX51D AZ150 yog HEM-DIP ALUMINI-Zinc Steel Alloy nrog ib txheej ntawm 55 feem pua ​​aluminium aluminium Cov tshuaj lom neeg muaj pes tsawg leeg ntawm DX51D AZ150 muaj cov tshuaj tiv thaiv zoo dua rau cua sov thiab xeb, nrog siab thermal refreathivity thiab conductivity.

Khoom Taw qhia

Khoom Taw qhia

 

DX51D muaj nyob rau hauv thicknesses ntawm0.45-3.00 hlithiab dav mus txog 1520 hli. DX52D muaj nyob rau hauv thicknesses ntawm 0.50-3.00 hli thiab dav mus txog 1520 hli. DX53D muaj nyob rau hauv thicknesses ntawm 0.50-3.00 hli thiab dav mus txog 1520 hli. DX54D muaj nyob rau hauv thicknesses ntawm 0.50-3.00 hli thiab dav mus txog 1520 hli.

 

Khoom npe
Galvanized sawb hlau
Qhov tuab
0.15mm-3.0mm
Lub hom phiaj
GB / JIS / DIN / EN / ASTM
Teem nqi
Q195, Q235, DX51D, SGCC, thiab lwm yam.
Nplaim
Txoj kev sib deev, chromate passivation
Tshuaj
Lub sau
Teem nqi
C %
SI%
Mn%
P %
S %
Q195
Tsawg dua los yog sib npaug rau 0.12
Tsawg dua los yog sib npaug rau 0.30
Tsawg dua los yog sib npaug rau 0.50
Tsawg dua los yog sib npaug rau 0.035
Tsawg dua los yog sib npaug rau 0.035
Q235
Tsawg dua los yog sib npaug rau 0.22
Tsawg dua los yog sib npaug rau 0.35
Tsawg dua los yog sib npaug rau 1.4
Tsawg dua los yog sib npaug rau 0.035
Tsawg dua los yog sib npaug rau 0.035
DX51D
Tsawg dua los yog sib npaug rau 0.12
Tsawg dua los yog sib npaug rau 0.50
Tsawg dua los yog sib npaug rau 0.60
Tsawg dua los yog sib npaug rau 0.1
Tsawg dua los yog sib npaug rau 0.045
SGCC
Tsawg dua los yog sib npaug rau 0.15
-
Tsawg dua los yog sib npaug rau 0.80
Tsawg dua los yog sib npaug rau 0.05
Tsawg dua los yog sib npaug rau 0.03
Txawj kho ub no
Ntiag tug
Teem nqi
Paib lub zog
MPa
Lub zog tensile
MPa
Elongation
Q195
Ntau dua los yog sib npaug rau 195
315-430
22%
Q235
Ntau dua los yog sib npaug rau 235
370-500
19%
DX51D
-
270-500
22%
SGCC
Ntau dua los yog sib npaug rau 205
Ntau dua los yog sib npaug rau 270
22%
Cov Ntawv Thov
Cov Khoom Siv Hauv Tsev, Cov Tsheb, Tsheb nkhaus, Cov Khoom Hlau Steel, Khoom,
Cov ntaub ntawv tsim tsev, thiab lwm yam.

 

Q: Thaum cov khoom tau txais los ntawm cov neeg siv khoom tsis ua raws li cov khoom lag luam lossis ntawv cog lus, koj yuav ua li cas?
Peb yuav them tus nqi rau txhua tus poob yam tsis muaj kev txaj muag.

 

Q: Ntev npaum li cas yog koj lub sijhawm khoom plig?
Feem ntau nws yuav siv sijhawm li ntawm 10 hnub yog tias cov khoom lag luam nyob hauv Tshuag, lossis nws yuav siv sijhawm li ntawm 25 hnub yog tias cov khoom yuav tsum tau customized.