1.0MM Cold Rolled Coil DC01
Siv teb:
|
tshuaj muaj pes tsawg leeg |
C | Mn | P | S |
|---|---|---|---|---|
| Min | - | - | - | - |
| Max | 0.12 | 0.6 | 0.045 | 0.045 |






Cim npe nrov: 1.0mm txias dov kauj dc01, Tuam Tshoj 1.0mm txias dov kauj dc01 manufacturers, lwm tus neeg, Hoobkas