JIS G3113 Saph400 Txias Rolled Steel Kauj

JIS G3113 Shap400 Txias Rolled Steel Chev yog qhov ua tau zoo dua qub hlau nrog cov khoom siv sib sib zog nqus, cov khoom siv hauv tsev, khoom siv hlau, thiab lwm yam

Khoom Taw qhia

Khoom Taw qhia

 

Cov khoom lag luam

JIS G3113 Shap400 Txias Rolled Steel Kauj ua nrog Japanese muaj cov qauv kev lag luam Nyiv (JIS-lub zog, High-ductility txias-rolled steel. Nws yog tsim nyog tshwj xeeb rau cov ntawv thov uas xav tau kev tsim kho kom zoo thiab nqus kev ua kom sib sib zog nqus.
Cov Khoom Siv Gnee Shap400 Rolled Steel Chev hauv ntau qhov kev qhia tshwj xeeb, thiab tuab, dav thiab ntev tuaj yeem kho tau raws li cov neeg siv khoom xav tau.
Shap400 Cr Txias Rolled Chev yog dav siv nyob rau hauv ntau cov liaj teb xws li tsheb tsim, cov khoom siv hauv tsev, thiab cov khoom siv hlau. Cov kev siv tshwj xeeb suav nrog cov tsev nyob hauv tsev, cov khoom siv hauv tsev, cov khoom siv hlau, thiab lwm yam.

Cov Ntaub Ntawv Khoom

JIS G3113 Saph400 Automotive Hlau Specificions

Teem nqi

Lub caij max (%)

Sap400

C

Si

Mn

P

S

0.21

0.30

1.40

0.030

0.025

Rau ALT

Nb

V

Ti

 

Ntau dua los yog sib npaug rau 0.010

       

Cov cuab yeej cuab tam ntawmSaph400 Tsheb Qauv Hlau Hlau Phaj:

Teem nqi

Elongation (dov kev taw qhia)%

No.5 Xeem

No.1a Xeem Daim

Ntau dua los yog sib npaug rau 1.6<2mm

Ntau dua los yog sib npaug rau 2.0<2.5mm

Ntau dua los yog sib npaug rau 2.5
<3.15mm

Ntau dua los yog sib npaug rau 3.15
<4.0mm

Ntau dua los yog sib npaug rau 4.0
<6.3mm

Ntau dua los yog sib npaug rau 6.3mm

 

Sap400

31

32

34

35

36

24

Teem nqi

Tensile lub zog n / mm2 min

Paib tau taw tes n / hli2

<6

Ntau dua los yog sib npaug rau 6<8mm

Ntau dua los yog sib npaug rau 8<14mm

Sap400

400

255

235

235

Khoom Zaub

JIS G3113 Saph400 Tsheb Hlau Qauv Hlau Chev

JIS G3113 SAPH400 Automobile Structural Steel Coil

 
Vim li cas thiaj xaiv GNEE

Gnee cov khoom tseem ceeb muaj cov xim sib xyaw ua xim hlau, cov kauj qia txhuas, galvanized steel cheel, thiab xim steel vuas, thiab xim pob zeb vuas.
GNE cov khoom tau raug xa tawm mus rau ntau lub tebchaws hauv ntiaj teb, suav nrog Tebchaws Europe, Tebchaws Asmeskas, Asmeskas, thiab lwm yam kev lag luam.

Yog tias koj muaj lus nug txog cov khoom lag luam uas muaj feem xyuam, thov hu rau peb.gi@gneesteel.com

Gnee Cov Neeg Siv Khoom

Gnee Customer visit

Gnee Chaw Lag Luam

Gnee Factory environment

Gnee ntim thiab xa khoom

 Gnee Packaging and shipping

Cov FAQ

Q.Why Xaiv GNee?
A.Ywith peb, koj yuav tau txais tus nqi sib tw tshaj plaws, lav tau zoo, lav tau xa khoom thiab tom qab muag cov kev pab.
Q. Koj puas muaj kev tswj hwm zoo?
A.yes, peb muaj peb tus kheej kev tswj xyuas kev nyab xeeb.
Q.What yog koj lub sijhawm coj ua?
A.Generally, peb lub sijhawm khoom xa tuaj yog nyob hauv 7-45 hnub.