Tsev-Xov xwm-

Ntsiab lus

Z600 Galvanized hlau

Apr 01, 2024

Z600 galvanized hlau

Z hauv lub npe sawv cev rau zinc, tab sis dab tsi txog 600? Tus lej ntawd yeej qhia tus lej ntawm grams ib square meter. Tus lej ntau dua, yog li ntawd, qhia tias txheej txheej tuab dua. Qhov tseeb, cov cuab yeej cuab tam gal ru tsev kuj muaj nyob rau hauv Z275 thiab Z450. Yog li Z600 yog qhov kev xaiv tuab tshaj plaws, tuaj ntawm 600 grams zinc txheej ib square meter.

 

GNEE Galvanized steel Z600 yog kub-dipped zinc-coated steel nrog spangled nto uas ua raws li AS/NZS 1397. Yam tsawg kawg nkaus lub zog yog G550 (550 MPa) los yog G300 (300 MPa), nyob ntawm qhov khoom. Cov txheej txheej tsawg kawg yog Z600 (600g / m2). Lub hauv paus hlau thickness yog 0.42mm los yog 0.60mm, nyob ntawm seb cov khoom.


GNEE STEEL kub muag zinc coated steel thickness

Txheej txheej Yam tsawg kawg nkaus txheej txheej, ob qhov chaw (g / m2) * Kev taw qhia tus nqi rau txheej thickness ntawm ib qhov chaw, feem ntau (μm)
Z100 100 7
Z140 140 10
Z180 180 13
Z200 200 14
Z225 225 16
Z275 275 20
Z350 350 25
Z450 450 32
Z600 600 42
gnee galvanised z600
Z600 yog galvanized
z600 galvanised
Z600 galvanized hlau

GNEE's Z600 galvanized steel muab txoj hauv kev zoo tshaj plaws los ua kom tau raws li qhov yuav tsum tau muaj rau kev tiv thaiv hlau uas tau teev tseg hauv tsab xov xwm tshiab ntawm National House Building Council's (NHBC) cov qauv tswj dej noo rau lub teeb steel framing nyob rau hauv cov tsev tshiab, nrog rau cov tsev, chav tsev, cov tub ntxhais kawm kev pab thiab tu tsev.Tiv tauj pebkawm ntxiv!

Xa kev nug