Kub - dipped galvanized steel chev
Nyem kom tau txais cov npe teev cov nqi hnub no!
QhiaGnee steelSab saum toj - ntawm - {line} Kab Galvanized Steel Co, tsim kom tau raws li cov qauv siab ntawm kev ua tau zoo thiab ua tau zoo. Engineered nrog precision thiab coated nrog ib txheej ntawm zinc, peb galvanized steel co tshuab roj muaj zog, ua rau lawv zoo tagnrho rau ntau cov ntawv thov.
Kub - dipped galvanized steel chev yog ib hom khoom siv steel uas tau sib xyaw nrog ib txheej ntawm kev tiv thaiv nws los ntawm kev corrosion. Cov txheej txheem cuam tshuam nrog tus hlau chev rau hauv da dej ntawm molten zinc, uas ua rau daim ntawv sib thooj metallurgical nruab nrab ntawm zinc thiab cov hlau.
Cov txheej no muab cov ruaj khov thiab ntev -} kav hlau, ua rau nws siv ntau yam xws li kev tsim kho, thiab kev tsim khoom lag luam.
-
Muaj Cov Hlau Qib
Peb galvanized steel co yog tsim nruj me ntsis raws li ANTM A653, thiab AS 1397 tus qauv. Hauv qab no yog cov muaj cov qauv steel thiab cov kws kho tshuab.
Cov khoom siv neeg kho tshuab ntawm cov hlau tsis tshua muaj cov hlau rau kev sib tsoo txias
| Kev tsim | Pub lub zog (MPA) |
Lub tensile lub zog (MPA) |
Elongation % min. |
||
|---|---|---|---|---|---|
| Qib hlau | Cov cim rau cov hom muaj txheej |
||||
| Hlau lub npe |
Hlau tus nab npawj |
||||
| DX51D | 1.0917 | + Z, + zf, + za, + zm, + az, + li, | – | 270 rau 500 | 22 |
| DX52D | 1.0918 | + Z, + zf, + za, + zm + AZ, + li | 140 txog 300 degree | 270 rau 420 | 26 |
Cov Khoom Siv Neeg Kho Tshuab ntawm Cov Hlau Rau Kev Tsim Kho
| Kev tsim | Cov Khoom Siv Neeg Kho Tshuab | ||||
|---|---|---|---|---|---|
| Qib hlau | Cov cim rau cov hom ntawm cov muaj yees | Pov thawj lub zog (MPA) min. |
Lub zog tensile (MPA) min. |
Elongation % min. |
|
| Hlau Npe Hlau | Hlau tooj | ||||
| S220Gd | 1.0241 | + Z, + ZF, + ZA, + ZM, + AZ | 220 | 300 | 20 |
| S250GD | 1.0242 | + Z, + zf, + za, + zm, + AZ, + li | 250 | 330 | 19 |
| S280Gd | 1.0244 | + Z, + zf, + za, + zm, + AZ, + li | 280 | 360 | 18 |
| S320gd | 1.0250 | + Z, + zf, + za, + zm, + AZ, + li | 320 | 390 | 17 |
| S350Gd | 1.0529 | + Z, + zf, + za, + zm, + AZ, + li | 350 | 420 | 16 |
| S390gd | 1.0238 | + Z, + ZF, + ZA, + ZM, + AZ | 390 | 460 | 16 |
| S420gd | 1.0239 | + Z, + ZF, + ZA, + ZM, + AZ | 420 | 480 | 15 |
| S450GD | 1.0233 | + Z, + ZF, + ZA, + ZM, + AZ | 450 | 510 | 14 |
| S550GD | 1.0531 | + Z, + ZF, + ZA, + ZM, + AZ | 550 | 560 | – |
Nyem kom tau txais cov npe teev cov nqi hnub no!