Nrhiav kev ntseeg siab galvanized steel phaj manufacturers hauv Suav teb? Koj twb tuaj rau qhov zoo lawm. Raws li lub Hoobkas ncaj qha nrog 20 xyoo ntawm kev tsim steel hlau, GNEE Steel muab cov nplooj ntawv ntawm lub Hoobkas nqi. Hauv phau ntawv qhia no, peb yuav hloov kho 2026 daim ntawv teev nqi tshiab thiab pab koj suav tag nrho cov nqi tsaws suav nrog kev thauj khoom thiab kev lis kev cai.

Galvanized steel phaj
Galvanized steel phajyog ib daim ntawv carbon steel coated nrog nyias txheej ntawm zinc los ntawm kub -dip galvanizing los yog electro-galvanizing txheej txheem. Cov txheej no muab kev tiv thaiv corrosion zoo heev, ua rau nws zoo tagnrho rau kev siv sab nraum zoov thiab chaw ntub dej.
Cov kev siv feem ntau suav nrog kev tsim kho lub ru tsev, cov khoom siv tsheb, cov khoom siv hluav taws xob, cov khoom siv ua liaj ua teb, thiab cov thawv xa khoom. Cov qib nrov suav nrog SGCC, DX51D, DX52D, thiab Q235, uas ua tau raws li cov qauv thoob ntiaj teb xws li ASTM A653 thiab EN 10346.
Chemical Composition ntawm GNEE Galvanized Steel Phaj
| Qib | C (%) | Si (%) | Mn (%) | P (%) | S (%) | Zn Txheej (g / m²) |
|---|---|---|---|---|---|---|
| SGCC | Tsawg dua lossis sib npaug li 0.12 | Tsawg dua los yog sib npaug li 0.05 | Tsawg dua lossis sib npaug li 0.60 | Tsawg dua lossis sib npaug li 0.045 | Tsawg dua lossis sib npaug li 0.045 | 60-275 |
| xwm 51d | Tsawg dua lossis sib npaug li 0.12 | Tsawg dua los yog sib npaug li 0.05 | Tsawg dua lossis sib npaug li 0.60 | Tsawg dua lossis sib npaug li 0.045 | Tsawg dua lossis sib npaug li 0.045 | 60-275 |
| Q235 | Tsawg dua los yog sib npaug li 0.20 | Tsawg dua los yog sib npaug li 0.35 | Tsawg dua lossis sib npaug li 1.40 | Tsawg dua lossis sib npaug li 0.045 | Tsawg dua lossis sib npaug li 0.045 | 60-275 |
Mechanical Properties ntawm Galvanized Steel Phaj
| Qib | Yield zog (MPa) | Tensile zog (MPa) | Elongation (%) |
|---|---|---|---|
| SGCC | Ntau dua lossis sib npaug li 140 | 270-350 | Ntau dua lossis sib npaug li 28 |
| xwm 51d | Ntau dua lossis sib npaug li 140 | 270-350 | Ntau dua lossis sib npaug li 28 |
| Q235 | Ntau dua lossis sib npaug rau 235 | 375-500 | Ntau dua lossis sib npaug li 26 |
2026 GNEE Galvanized Steel Phaj Nqe Ntau
Tus nqi ntawm galvanized steel phaj txawv raws li thickness, txheej hnyav, thiab txiav txim kom muaj nuj nqis. Hauv qab no yog 2026 lub Hoobkas nqi daim ntawv teev npe rau GNEE Steel cov khoom:
| Thickness (hli) | Qhov hnyav (g / m²) | Nqe (USD/ton) | MOQ (tons) |
|---|---|---|---|
| 0.3-0.5 | 60-120 | $850-$920 | 25 |
| 0.6-1.0 | 120-180 | $820-$880 | 25 |
| 1.1-2.0 | 180-275 | $790-$850 | 25 |
| 2.1-4.0 | 275 | $760-$820 | 25 |
Txhua tus nqi suav nrog cov ntim khoom txheem (hiav txwv-cov ntoo pallets tsim nyog) thiab siv tau rau Q2 2026. Rau kev txiav txim ntau tshaj 100 tons, hu rau peb pab neeg muag khoom kom txo nqi tshwj xeeb.
Yuav Ua Li Cas Sau Tag Nrho Cov Nqi Tshaj Tawm
Txhawm rau pab koj npaj koj cov peev nyiaj, peb tau ua kom yooj yim rau kev xam tus nqi tsaws:
Tus nqi khoom: Raws li daim ntawv teev npe saum toj no thiab koj cov xaj kom muaj nuj nqis
Tus nqi thauj khoom: Kwv yees li ntawm $ 80- $ 120 / ton (nws txawv ntawm qhov chaw nres nkoj)
Kev lis kev cai: Nyob ntawm koj lub teb chaws txoj cai ntshuam tariff (feem ntau 5% -15%)
Lwm Tus Nqi: Kev tuav pov hwm (0.3% ntawm tus nqi khoom) thiab tus nqi tuav ($ 50- $ 100 / xaj)
Piv txwv li: 50 tons ntawm DX51D (1.0mm, 180g / m²) rau Rotterdam:
Tus nqi khoom: 50 tons × $850/ton=$42,500
Tus nqi thauj khoom: 50 tons × $ 100 / ton=$ 5,000
Kev lis kev cai: $42,500 × 8%=$3,400
Tus nqi tsaws tag nrho: $42,500 + $5,000 + $3,400 + $75 (kev pov hwm)=$50,975
GNEE Steel muab siab -zoogalvanized steel phajnrog cov nqi sib tw thiab txhim khu kev xa khoom. Txawm hais tias koj xav tau qhov ntau thiab tsawg lossis kev cai tshwj xeeb, peb lub Hoobkas tuaj yeem ua tau raws li koj xav tau. Hu rau peb hnub no kom tau txais kev tsocai pub dawb thiab kev txhawb nqa - cia peb tsim koj qhov project ua ke!
- Muaj Steel Qib
|
Txuj |
Qib |
C |
Si |
Mn |
P |
S |
Ti |
|
Kev Ua Txhaum Cai Suav Standard |
DX51D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
DX52D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
|
DX53D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
|
DX54D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
|
DX56D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
|
DX57D+Z |
0.12 |
0.50 |
0.60 |
0.100 |
0.045 |
0.30 |
|
|
Kev Ua Txhaum Cai Japanese Standard |
SGCC |
0.15 |
0.50 |
0.80 |
0.050 |
0.030 |
0.025 |
|
SGCD1 |
0.12 |
0.50 |
0.60 |
0.040 |
0.030 |
0.025 |
|
|
SGCD3 |
0.08 |
0.50 |
0.45 |
0.030 |
0.030 |
0.025 |
|
|
SGCD4 |
0.06 |
0.50 |
0.45 |
0.030 |
0.030 |
0.025 |
|
|
Rau Cov Qauv Japanese Standard |
TIAB SA 340 |
0.25 |
0.50 |
1.70 |
0.200 |
0.035 |
0.025 |
|
SIB 400 |
0.25 |
0.50 |
1.70 |
0.200 |
0.035 |
0.150 |
|
|
TIAB SA 490 |
0.30 |
0.50 |
2.00 |
0.200 |
0.035 |
0.025 |
|
|
TIAB SA 510 |
0.30 |
0.50 |
2.50 |
0.200 |
0.035 |
0.025 |
|
|
Rau Cov Qauv AISI Standard |
S220GD + Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.025 |
|
S250GD + Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.025 |
|
|
S280GD + Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.025 |
|
|
S320GD + Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.025 |
|
|
S350GD + Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.150 |
|
|
S550GD + Z |
0.20 |
0.60 |
0.70 |
0.100 |
0.045 |
0.150 |
Thov daim ntawv ceeb toom cov khoom siv kho tshuab + SGS daim ntawv pov thawj