Thaum lub Cuaj Hlis 10, 2024, GNEE tau xa tag nrho 349 tons ntawmSPCC txias dov steel strip coilsrau cov neeg siv khoom Thaib.

SPCC txias-kuav los tiag steel strips xa los ntawm GNEE yog tsim nruj me ntsis raws li cov kev cai ntawm Thaib cov neeg muas zaub. Lawv yog cov khoom siv zoo heev thiab cov lus qhia meej thiab tau siv dav hauv kev tsim tsheb, kev tsim khoom siv hauv tsev, precision machinery thiab lwm yam.

Thaum lub sijhawm xa khoom no, cov neeg siv khoom Thaib thawj zaug sim cov khoom siv kho tshuab ntawm cov khoom. Los ntawm lub tshuab kuaj tensile kev tshaj lij, cov kws tshuaj ntsuam xyuas nruj me ntsis ntsuas cov cim tseem ceeb ntawm cov hlau strips, xws li lub zog tawm los, lub zog tensile thiab cov yas sib piv. Cov txiaj ntsig tau pom tias cov khoom siv kho tshuab ntawm cov khoom ntawm SPCC txias-kuav los tiag steel strips ua tau raws li lub teb chaws thiab kev lag luam cov qauv, tag nrho lav lawv cov kev ruaj ntseg thiab kev ntseeg siab thaum lub sij hawm tom qab ua thiab siv. Tsis tas li ntawd, cov kws tshuaj ntsuam xyuas qhov ua tiav ntawm qhov kawg, flatness thiab seb puas muaj qhov tsis xws luag xws li cov kab nrib pleb thiab kev suav nrog ntawm cov hlau strips ib los ntawm ib qho.

Cov neeg siv khoom Thaib tau hais tias SPCC txias-kuav los tiag steel strips muab los ntawm GNEE yog cov khoom zoo thiab ua tau raws li lawv cov kev xav tau ntau lawm. Qhov kev koom tes no tsis yog tsuas yog ua rau kev nkag siab thiab kev ntseeg siab ntawm ob tog, tab sis kuj tau tsim lub hauv paus ruaj khov rau kev sib pauv lag luam ntau dua yav tom ntej.