Kub Dipped GL Galvalume Steel Coils (Aluzinc - GL)
Peb muab cov khoom zookub dipped galvalume steelntawv nyob rau hauv coils los ntawm kev coated steel manufacturers nyob rau hauv Suav teb nrog cov kev pab zoo tshaj plaws.
Qhov saum npoo ntawmgalvalume steel ntawvnta lub hnub qub-zoo, du thiab tiaj, nrog cov xim nyiaj ua xim thawj. Nws cov qauv tshwj xeeb plating tuaj yeem ua tau zoo corrosive -proof.
SPECIFICATION
| STANDARD | JIS G3321, ASTM A792M / A924M lossis sib npaug |
| COATING MASS | AZ30-Z150 |
| NTAU TSHAJ | Me Spangle, Tsis tu ncua Spangle thiab Loj Spangle (Ntau xim muaj ntsuab, xiav, liab thiab kub) |
| KEV KHO SIAB | Chromated / Unchromated Treatment, Oiled lossis Resin Coated (Anti Finger Print), Qhuav |
| TSEEM CEEB | Kev Kho Mob, Oiled lossis Resin Coated (Anti Finger Print thiab Non Anti Finger Print) |
Qhov zoo:
Muaj zog corrosion kuj, 3 npaug ntawmgalvanized steel ntawv.
Qhov ntom ntawm 55% aluminium yog me dua qhov ntom ntawm zinc. Thaum lub luj yog tib yam thiab lub thickness ntawm lub plating txheej yog tib yam, thaj tsam ntawm cov galvalume steel ntawv yog 3% los yog loj tshaj li ntawm cov galvanized steel ntawv.
GL Coil Test:
nruj me ntsis raws li txheej thickness ntsuas, hardness testing (miv hardness, khawb hardness), sim flexibility (impact, ncej khoov, T khoov, khob kos duab, stretch), adhesion test (kos khawb), degree ntawm curing test (iav hloov mus kuaj, Kev ntsuas cov kuab tshuaj tiv thaiv, kev ntsuas kub qhuav), lwm yam kev ntsuas kev ua tau zoo (Kev ntsuas qhov ntsuas qhov ntsuas, ntsuas qhov ci, ntsuas qhov tsis zoo, tshuaj lom neeg tsis kam, ntsuas kev puas tsuaj, kev sim poob, coefficient ntawm kev sib txhuam kev xeem).
Peb muab cov khoom zoo raw khoom, hnub xa khoom sai, kev pabcuam thiab pheej yig tus nqi.Tiv tauj pebtam sim no!
Hais txog GNEE STEEL:
GNEE STEEL Lub Tuam Txhab yog lub tuam txhab kev tshaj lij hlau ua ke nrog kev tshawb fawb, kev tsim kho, tsim khoom, muag thiab kev pabcuam. Nws muaj yim ceg, nrog rau txhua xyoo muag ntawm ze li ntawm 1 billion thiab txog 280, 000 tons ntawm hlau. Nws nyob hauv Anyang, Henan, nrog kev thauj mus los yooj yim.