Tinplate is a sheet with a layer of metallic tin on the surface of steel sheet. This treatment is designed to provide excellent corrosion resistance, paintability, weldability, as well as processability and strength while maintaining a bright appearance. Tinplate, also known as tinplate, is made by electroplating a layer of high-purity tin (Sn>99.8%) ntawm cov pa roj carbon tsawg.
Cov ntawv no tsis yog tsuas yog tsis muaj tshuaj lom thiab tsis muaj ntxhiab, tab sis kuj muaj qhov ci ntsa iab. Nws lub luag haujlwm tseem ceeb yog tiv thaiv corrosion thiab xeb. Kev tsim cov txheej txheem ntawm tinplate suav nrog dov, pickling, txias dov, electrolytic tu annealing, flattening, trimming, thiab ces ntxuav, electroplating, mos melting, passivation kev kho mob thiab oiling, thiab thaum kawg shearing rau hauv cov khoom tiav. Lub tin txheej kuj tuaj yeem siv los ntawm kub-dip plating. Txawm hais tias txoj kev no siv ntau npaum li cas ntawm cov tin thiab cov tin txheej yog thicker, nws tsis xav tau kev kho kom huv.

chrome-platedtxheej yog cov khoom siv tsis yog amphoteric thiab tsim nyog rau ntim cov ntsiab lus alkaline xws li detergents thiab pigment dispersants.
Tsis tas li ntawd, muaj chrome-plated phaj, uas yog tsim los ntawm electroplating ib tug hlau chromium txheej thiab ib tug chromium oxide txheej nyob rau saum npoo ntawm cov hlau sawb. Nws kuj muaj cov xim zoo nkauj zoo nkauj heev thiab zoo heev corrosion kuj. Chrome-plated sheet coil yog hais txog lub phaj hlau nrog txheej txheej ntawm chrome rau ntawm qhov chaw, uas yog siv los tiv thaiv qhov chaw ntawm cov hlau phaj los ntawm corrosion thiab txuas nws lub neej kev pab cuam.
Qhov zoo ntawm chrome-plated daim hlau
Cov xim pleev xim zoo heev: Cov xim nplaum yog ntau dua li cov tinplate, thiab tuaj yeem siv los tsim DRD cov kaus poom thiab cov kaus poom kua nplaum.
Kev kub siab denaturation kuj zoo heev: kub kub ua hauj, tsis muaj xim, thiab tsis deterioration ntawm cov khoom siv.
Cov tshuaj sulfide zoo heev: cov hlau chromium txheej muaj cov tshuaj sulfide zoo thiab tsim nyog rau cov kaus poom ntawm cov khoom noj muaj protein ntau xws li ntses
Kev tiv thaiv zoo heev rau filamentous corrosion: Zoo heev tiv thaiv filamentous corrosion nyob rau hauv cov xim zaj duab xis
Zoo heev alkali tsis kam; chrome-plated txheej yog cov khoom siv tsis yog amphoteric thiab tsim nyog rau ntim cov ntsiab lus alkaline xws li detergents thiab pigment dispersants.

Tinplate

 