Muaj qee qhov sib txawv ntawm cov ntaub ntawv thiab kev tsim khoom ntawm SGCC thiab SGHC kub-dip galvanized steel nplooj ntawv, raws li hauv qab no:
Khoom thiab npe:
SGCC: S sawv rau Hlau, G sawv rau Galvanized, C sawv rau Txias, thiab plaub C sawv rau Common. Yog li ntawd, SGCC stands rau kub-dip galvanized nyias txias-kuav los tiag steel sheet1.
SGHC: S kuj sawv cev rau Hlau, G sawv rau Galvanized, tab sis H sawv rau Kub, thiab plaub C kuj sawv rau Common. Yog li ntawd, SGHC yog hais txog kub-dip galvanized nyias kub dov steel sheet1.
Kev tsim khoom:
SGCC: Nws txais cov txheej txheem txias dov, uas yog, cov ntawv hlau yog dov los ntawm lub tshuab dov ntawm chav tsev kub kom ua tiav qhov xav tau tuab thiab loj. Cov ntawv txias-kuav los tiag steel ntawv muaj qhov zoo ntawm qhov zoo thiab qhov siab qhov tseeb, tab sis lawv cov kev ua tau zoo yuav ua rau me ntsis qis dua ntawm cov ntawv kub dov steel1. SGHC: Nws txais cov txheej txheem kub dov, uas yog, cov ntawv hlau yog dov los ntawm lub tshuab dov ntawm qhov kub thiab txias. Tej zaum yuav muaj qee yam ntawm cov hlau oxide nyob rau saum npoo ntawm cov ntawv kub-kuav los tiag, tab sis kev ua haujlwm zoo, thiab nws yog qhov tsim nyog rau qee lub sijhawm uas yuav tsum muaj zog dua thiab tawv. Daim ntawv thov: Vim muaj cov txheej txheem tsim khoom sib txawv thiab kev ua haujlwm, SGCC thiab SGHC kub-dip galvanized steel nplooj ntawv kuj tseem sib txawv hauv lawv cov kev siv. Tab sis feem ntau, lawv yog ob qho tib si kub-dip galvanized steel ntawv nrog zoo heev corrosion kuj thiab zoo nkauj zog, thiab yog dav siv nyob rau hauv kev tsim kho, khoom siv hauv tsev, tsheb, tsheb thauj mus los thiab lwm yam kev lag luam.