Dab tsi yog Lwm Lub Npe Rau Cold Rolled Steel?

Dec 03, 2025

Lwm lub npe rau txias dov steel yog dab tsi?

 

Txias-rolled steel yog paub los ntawm ob peb lwm lub npe thiab cov qauv tsim thoob ntiaj teb cov qauv, ua rau nws tseem ceeb rau cov neeg yuav khoom, cov kws tsim khoom, thiab pab pawg muag khoom kom nkag siab txog nws cov lus sib hloov. Hauv kev lag luam steel, txias-rolled steel feem ntau hu ua CR steel, txias-txo steel, CRS, txias-rolled sheet (CRS), lossis txias-rolled coil (CRC). Hauv cov cheeb tsam sib txawv, nws kuj tseem yuav raug txheeb xyuas los ntawm cov lej tshwj xeeb xws li DC01, DC03, DC04, DC05, DC06, thiab DC07 hauv EN 10130 tus qauv, lossis SPCC raws li JIS G 3141 tus qauv.Cov npe lwm yam pab faib cov khoom raws li daim ntawv thov, qhov zoo, thiab kev ua haujlwm zoo.

 

1. Kev sib piv qib siab

Table 2. DC01–DC07 Qib Kev Ua Haujlwm

Qib Formability Yield zog Daim ntawv thov tseem ceeb
dc01 ua ★★☆☆☆ Nruab nrab Txee, brackets, profiles
dc03 ua ★★★☆☆ qis Automotive qhov chaw yuav tsum tau kos duab
dc04 ua ★★★★☆ Tsawg Cov khoom siv vaj tse
dc05 ua ★★★★☆ Tsawg heev Sib sib zog nqus- kos cov khoom
dc06 ua ★★★★★ Ultra - Tsawg Roj tank, cov duab complex
dc07 ua ★★★★★ qis tshaj Precision multi-theem sib sib zog nqus kos duab

Qhov kev nce qib ntawm DC01 mus rau DC07 qhia txog kev ua kom muaj zog ntxiv thiab txo qis zog.

 

2. Kev faib tawm ntawm Cold Rolled Steel Qib

EN 10130 tus qauv siv dav hauv kev lag luam thoob ntiaj teb suav nrog cov qib tseem ceeb hauv qab no:

Table 1. Txias Rolled Steel Qib Classification

Qeb Qib Kev piav qhia
Kev Lag Luam Zoo dc01 ua General forming thiab dabtsi yog khoov
Kev kos duab zoo dc03 ua Haum rau kev kos duab nruab nrab
Deep Drawing Zoo DC04, DC 05 Zoo dua ductility, tsis tshua muaj zog tawm los
Ultra-Drawing tob dc06, ua 07 Maximum elongation rau complex duab

Cov pawg no pab txiav txim siab seb qib twg tsim nyog rau cov ntawv thov xws li kev khoov yooj yim mus rau siab -xav tau ntau- theem tsim.

 

3. Cov qib khoom sib npaug thoob ntiaj teb

Cold rolled steel muaj qhov sib npaug hauv lwm cov qauv loj xws li JIS hauv Nyiv, ASTM hauv Tebchaws Meskas, thiab ISO thoob ntiaj teb.

Table 3. Ntiaj teb no sib npaug ntawm Cold Rolled Steel Qib

EN Qib JIS sib npaug ASTM sib npaug Sau ntawv
dc01 ua SPCC A1008 CWJ Kev lag luam hlau
dc03 ua SPCD A1008 DS Daim duab hlau
dc04 ua SPCE A1008 DDS Sib sib zog nqus nqus hlau
dc05 ua SPCE-SD A1008 UAS Kev kos duab sib sib zog nqus
dc06 ua SPCF A1008 EDDS+ Ntxiv - kos duab sib sib zog nqus
dc07 ua SPCE-SD (ze tshaj) EDDS Ultra sib sib zog nqus kos duab

Cov lus no pab cov engineers hloov cov ntaub ntawv thaum qee cov qib tsis muaj nyob hauv khw hauv zos.

 

Peb lub tuam txhab tseem tuaj yeem muab cov khoom txias txias hauv qab no - dov steel qib:
DC01 - Tsim los rau cov txheej txheem tsim cov txheej txheem xws li khoov, embossing, hlaws thiab cov qauv kos duab.
DC03 - Npaj rau kev thov ntau daim ntawv thov, suav nrog kev kos duab sib sib zog nqus thiab ntau qhov profile.
DC04 - Haum rau cov ntawv thov uas xav tau qib siab ntawm formability.
DC05 - Ib qho sib sib zog nqus- qib kos duab tsim kom tau raws li qhov yuav tsum tau ua siab heev.
DC06 - Ib qho tshwj xeeb sib sib zog nqus- qib kos duab tsim rau qhov kev xav tau siab tshaj plaws hauv kev ua kom txias.
DC07 - Ib qho kev sib sib zog nqus tob heev -qib duab kos rau kev ua haujlwm hnyav thiab nyuaj heev.