Yuav ua li cas koj thiaj paub thiab kho cov kev tsis xws luag saum npoo ntawm galvanized steel coils? SGCC SGCC SGCCH DX51D

Nov 19, 2025

Nto qhov tsis xws luag & kho cov kev ua haujlwm

 

Nyem kom tau txais cov npe teev cov nqi hnub no!

Kub dipped galvanized steel coil yog qhov tseem ceeb hauv kev lag luam uas xav tau ntev}}} durability tiv thaiv corrosion, tshuab hluav taws xob ntev, thiab cov kev daws teeb meem. Cov coils galvanized no tau siv dav siv hauv kev tsim kho, tsheb, hvac, kev ua liaj ua teb, thiab cov ntawv thov kev lag luam.

 

Zinc co coating ua raws li kev thaiv tawm tsam ya raws, ntsev, thiab corrosive tshuaj, thaum tseem muab tshuaj tua kab mob kev tua kab yog tias yog cov txheej puas lawm. Qhov no ua kom pom tseeb cov steel cov khoom tseem muaj kev tiv thaiv txawm tias hauv qab kev puas tsuaj lossis khawb. Coils tuaj yeem ua tiav rau hauv cov ntawv txheeb, ib daim hlab, cov kav dej, thiab lwm daim ntawv, ua rau kub daim hlau loj heev rau ntau yam kev siv khoom.

Hot Dipped Galvanized Steel Coil Dx53D+Z

 

Txawm tias muaj kev sib tua zoo,Galvanized Steel Chev Cov Khoom Sivtej zaum yuav ntsib superficial hloov pauv thaum cia lossis thauj khoom:

 

Pom cov nyhuv

Kev kom

Kev ua zog

Lub teeb dawb tsis meej (nyias, hmoov)

Noo noo ntawm cov ntawv txheeb lossis hws

Tsis muaj kev nqis tes ua; ZINC converts los tiv thaiv carbonate dhau sijhawm

Cov khoom tso nyiaj dawb dawb (tuab, ua plusty)

Kev nthuav dav ntev heev

Tshem tawm nrog txhav txhav ua ntej txhuam; Kos txheej txheej tuab

Dub Staining nrog Hmoov

Thaum Ntxov Dinc Corrosion

Soj ntsuam tuab; feem ntau tsis muaj teeb meem

Xeb liab

Cov Tov Txheej

Kho lossis hloov cov khoom cuam tshuam

 

Cov kev ntsuas no kom muaj kev ncaj ncees thiab ntev -} lo lus ua tau zoo rauKub dipped Galvanized Steel Coils.

 

Hot Dipped Galvanized Steel Coil Dx53D+Z

Cov lus qhia tshwj xeeb:

 

Lub hom phiaj

JIS G3302, E10147, ASTM A653M

Teem nqi

Commerical: SGCC, SGCH, DX51D

Kev sib sib zog nqus: DX52D, DX52D, DX53D, DX54D, DDS, SGCD, SGC

Kev los ntawm thiab cov hlau structrual: S280GD, S320Gd, S350GD, S400GD, S500GD, S550GD

Zinc Txheej

Z30-400G/M2, G30, G60,G90, Z10, Z12,Z27

Kab Kab Tsiaj

Xoom spangle, me me kab plaub, ib txwm ua, loj spangle

Nto Kho

Chromated, oiled, tsis muaj - roj

Kev nyuaj

Sofy, ib nrab nyuaj, tag nrho nyuaj, g550

Qhov tuab

0.11-4.00mm

Qhov dav

20-1800 hli

Coil hnyav

Coil hnyav

Coil sab hauv taub

508mm lossis 610 hli

Lub thawv

Txheem Seaworthy Exporting Ntim

 