Dec 29, 2025

galvanized hlau

 

DX53D Z80 kub dip 1.2 hli tuab galvanized steel kauj yog cov khoom sib sib zog nqus nqus cov khoom tsim raws li EN 10346. Nws siv siab -zoo qis- carbon txias dov hlau ua cov khoom siv hauv paus thiab siv cov txheej txheem Z80 zinc txheej los ntawm kev kub kub -dip galvanizing. Qhov kev sib xyaw ua ke no muab cov hlau zoo tshaj plaws tsim kev ua tau zoo, ruaj khov txhua yam tus cwj pwm thiab txhim khu kev tiv thaiv corrosion.

 

Lub thickness 1.2 hli muab cov qauv rigidity thaum seem hloov tau txaus rau txoj kev sib sau. Z80 txheej muab kev tiv thaiv zoo rau kev pabcuam sab hauv tsev thiab sab nraum zoov, ua cov khoom siv no dav siv hauv kev tsim khoom, khoom siv hluav taws xob, HVAC systems, steel rooj tog thiab precision hlau fabrication.

 

galvanized steel coil

  • Tshuaj muaj pes tsawg leeg

Element C Mn P S Al
Max % 0.08 0.45 0.030 0.025 0.015

 

  • Mechanical Properties

Khoom Tus nqi
Yield zog 140-220 MPa
Tensile zog 270-380 MPa
Elongation Ntau dua lossis sib npaug li 36%
Hardness Tsawg dua lossis sib npaug li 110 HV

 

DX53D Z80 1.2mm galvanized steel kauj ua tau zoo tshwj xeeb hauv cov kab ntau lawm uas qhov tseeb qhov tseeb thiab rov ua dua yog qhov tseem ceeb. Cov khoom ntws zoo thaum lub sij hawm stamping thiab dabtsi yog khoov, minimizing springback thiab cuab yeej hnav. Nws zoo ib yam nto zoo kuj txhim kho painting adhesion thiab zaum kawg khoom tsos.

 

Manufacturers tau txais txiaj ntsig los ntawm:

  • Txo txoj kev ua tsis xws luag
  • Tsawg tus nqi seem
  • Txhim kho qhov ntsuas qhov ntsuas
  • Ntev tooling lub neej
  • Cov txheej txheej ruaj khov tom qab deformation

 

DX52D vs DX53D hauv 1.2mm Thickness

 

Feature xwm 52d xwm 53d
Elongation Ntau dua lossis sib npaug li 30% Ntau dua lossis sib npaug li 36%
Sib sib zog nqus kev ruaj ntseg Zoo Zoo heev
Nto tiav tom qab tsim Zoo Superior
Kev Ua Tau Zoo Siab Siab heev

 

Kev tsim khoom Case

Ib lub chaw tsim khoom ntawm cov khoom siv hluav taws xob thaum chiv thawj siv DX52D galvanized steel ntawm 1.2 hli thickness. Thaum lub sijhawm ua haujlwm folding nyuaj, cov kab nrib pleb me me feem ntau tshwm nyob ib puag ncig kaum radii. Tom qab hloov mus rau DX53D Z80 galvanized steel kauj, qhov tsis xws luag poob los ntawm 31%, kev sib koom ua ke tau zoo dua qub, thiab cov khoom siv tau nce ntau dua 15%.

 

Hom Specifications

 

Thickness (hli) Dav (mm) Coil Luj (MT)
1.2 600–1500 3–25

 

Zinc Txheej Qhov hnyav (g / m²) Kev Pabcuam Ib puag ncig
Z80 80 Sab hauv & lub teeb sab nraum zoov
Z120 120 General sab nraum zoov
Z275 275 Nyuaj sab nraum zoov

 

  • DX53D Galvanized Steel Coils

Specification Metric (mm) Imperial (ntev)
Thickness 0.3-3.0 hli 0.012-0.118 hli
Dav 600-1500 hli 23.62-59.06 Nws

 

  • DX53D Galvanized Steel Sheets

Specification Metric (mm) Imperial (ntev)
Thickness 0.3-3.0 hli 0.012-0.118 hli
Dav 600-1500 hli 23.62-59.06 Nws
Ntev 1000-6000 hli 39.37-236.22 nyob rau hauv

 

  • DX53D Galvanized Steel Strips

Specification Metric (mm) Imperial (ntev)
Thickness 0.3-3.0 hli 0.012-0.118 hli
Dav 20-600 hli 0.79-23.62 hli

 

GNEE STEEL muab DX53D Z80 kub dip 1.2mm galvanized steel kauj nrog kev tswj nruj, kev tswj txheej txheej thiab txhim khu kev qha txhua yam. Peb cov kev pabcuam xa tawm, cov khoom siv ruaj khov thiab kev txhawb nqa kev pabcuam pab cov neeg siv khoom txhim kho kev tsim khoom thiab txo qis kev pheej hmoo ua haujlwm.

 