Khoom Description
DX51D+AZthiabDC51D + AZyog ob leegkub-dip galvalume steel qibnrog 55% Al-43.4% Zn-1.6%Si txheej, tab sis lawv txawv ntawm cov hauv paus chiv keeb, cov qauv siv tau, thiab tsim kev sib xws-DX51D + AZ ua raws EN 10346 nrog ntau yam kev xaiv substrate, thaum DC51D + AZ ua raws li Suav Q / BQB a 42tsau txias- dov DC01 substrate. Raws li tus thawj coj galvalume steel tsum, GNEE STEEL qhia meej cov kev sib txawv tseem ceeb no los pab koj xaiv cov qib zoo rau koj qhov project.
- DX51D+AZ: Ib qho European- qauv galvalume steel qib rau kev sib sau txias, qhov twg "D"=tiaj tus hlau rau kev sib sau txias, "X" =indefinite dov lub xeev(tshaj nrog ob qho tib si kub-rolled DD11 thiab txias- dov DC01 substrates), "51"=qib series tooj, qhov thib ob "D"=kub-dip coated, thiab "+AZ"=Al-Zn alloy txheej.
- DC51D + AZ: Suav - qauv galvalume steel qib rau kev sib sau txias, qhov "C" =txias- dov substrate nkaus xwb(tso DC01 qis- carbon txias- dov steel puag), nrog tib txheej txheej (+ AZ) thiab cov cuab yeej cuab tam raws li DX51D + AZ.
Qhov tseem ceeb Standard & Substrate sib txawv
Qhov tseem ceeb tshaj qhov sib txawv yog nyob rau hauvtswj cov qauv thiab substrate sib xws, ncaj qha cuam tshuam cov khoom ruaj khov thiab kev siv thoob ntiaj teb.
| Cov khoom sib piv | DX51D+AZ | DC51D + AZ |
|---|---|---|
| Siv tau Standard | TS EN 10346 (EU, 2015) | Q/BQB 425 (Suav teb) |
| Hom substrate | Yeem: Kub- dov (DD11) lossis Txias- dov (DC01) | Kho: Txias- dov DC01 nkaus xwb |
| Cov ntsiab lus carbon substrate | 0.06-0.12% (kuj hloov los ntawm substrate) | 0.08–0.12% (tso qis -carbon) |
| Kev lees txais thoob ntiaj teb | Siab (siv dav hauv EU, Southeast Asia, Middle East) | Regional (tsuas yog rau cov haujlwm hauv Suav teb) |
| Dimensional kam rau ua | ± 0.02 hli (EN 10346 nruj kam rau ua) | ± 0.03mm (Q / BQB 425 tus qauv kam rau ua) |
Mechanical Property Performance
Ob qib sib npaugmechanical khoom pibraws li EN 10346, tab sis DC51D + AZ muaj kev ua tau zoo dua qub vim nws qhov txias txias -rolled substrate.
Core Mechanical Properties (Cov Nqi Zoo Tshaj):
Yield Strength (Re):140-220MPa (tsawg dua lossis sib npaug rau 220MPa tus qauv txwv)
Tensile zog (Rm):270-350MPa
Elongation (A80):Ntau dua lossis sib npaug li 22% (tsawg kawg rau kev sib sau txias)
Hardness:PIB 50–65
Daim Ntawv Qhia Qhov Sib Txawv:DX51D + AZ nrog kub - dov DD11 substrate muaj5-8% qis elongationtshaj DC51D + AZ, ua DC51D + AZ zoo dua rau txoj kev khoov los yog stamping txheej txheem.
Galvalume txheej yam ntxwv
Ob qib feature qhovtib lub siab -kev ua tau zoo AZ txheej(55% Al-43.4% Zn-1.6% Si), kev lag luam tus qauv kub rau corrosion kuj.
Txheej Core Parameters:
Txheej Nyhav:AZ30–AZ150 g/m² (ob -sided; customizable mus txog AZ275)
Corrosion Resistance:1.
Thaum tshav kub kub Resistance:Kev siv txuas ntxiv mus txog 315℃(luv-lub sij hawm mus txog 400 degree) tsis muaj txheej txheej los yog tev
Surface Appearance:Bright silver matte tiav (reflectivity Ntau dua lossis sib npaug li 75% rau pom lub teeb)
Daim Ntawv Thov Scenario: Yuav Xaiv Qhov twg?
DX51D+AZ: Qhov zoo tshaj plaws rau Kev Ua Haujlwm Ntiaj Teb & Nqis - Siv tau zoo
Export tsim: ru tsev, phab ntsa panels, corrugated ntawv rau EU, Southeast Asian, los yog Middle Eastern tej yaam num
General txias-tsim qhov chaw: qhov cua qhov ducts, culverts, thiab qis- cov khoom muaj zog
Tus nqi- daim ntawv thov nkag siab: Kub- kev xaiv cov txheej txheem dov txo cov nqi khoom los ntawm 8–12%
DC51D + AZ: Qhov zoo tshaj plaws rau siab -Precision Forming & Suav Domestic Projects
Complex stamping: Cov khoom siv hauv tsev plhaub (cov tub yees rov qab vaj huam sib luag, lub tshuab cua txias), cov khoom siv hluav taws xob
High-kev tsim kho qhov tseeb: Cov kab hlau rhuav phab ntsa, hnub ci mounting brackets yuav tsum tau tswj kom nruj
Automotive qhov chaw: Tshem tawm cov cua sov, cov tais roj teeb (siab kub thiab corrosion kuj)
GNEE STEEL's Galvalume Steel Advantage
Ntawm GNEE STEEL, peb muab ob qho tib siDX51D + AZ thiab DC51D + AZ galvalume steel coils / ntawvnrog nruj zoo tswj:
Thickness: 0.2-2.0mm, dav: 1,000-1,500mm (customizable)
Certified rau EN 10346 thiab Q / BQB 425, nrog tag nrho cov ntawv pov thawj zeb xeem (MTC)
Nto xaiv: Chromium-dawb passivated, ntiv tes{1}}resistant, oiled/unoiled
Kev xa khoom thoob ntiaj teb: EXW, FOB, CIF cov ntsiab lus, nrog 10-tuj MOQ thiab cov qauv xa tawm
Cov lus nug nquag nug (FAQ)
Q1: Puas yog DX51D + AZ thiab DC51D + AZ hloov pauv tau?
A1: Ib nrab interchangeable rau yooj yim txias sib sau, tab sis DC51D + AZ yog qhov zoo dua rau kev stamping nyuaj vim nws qhov txias txias -rolled substrate thiab zoo ib yam elongation. DX51D + AZ yog qhov zoo dua rau cov phiaj xwm xa tawm thoob ntiaj teb uas xav tau EN 10346 ua raws.
Q2: Tus nqi sib txawv ntawm ob qib yog dab tsi?
A2: DC51D + AZ feem ntau yog3-5% kim duatshaj DX51D+AZ (kub- dov substrate) vim nws qhov txias txias - dov DC01 puag. DX51D + AZ (txias- dov substrate) yog tus nqi ze li ntawm DC51D + AZ.
Q3: DX51D + AZ puas tuaj yeem siv rau hauv qhov chaw siab - qhov kub thiab txias?
A3: Yog. Ob qib muaj tib yam315℃nruam kub tsis kam(luv-lub sij hawm mus txog 400℃) vim qhov zoo tib yam 55%Al-Zn-Si txheej, haum rau lub qhov cub plhaub, cov khoom tso tawm, thiab siab - kub ducting.
Q4: Qib twg zoo dua rau kev tsim kho ntug dej hiav txwv?
A4: Ob leeg muaj kev tiv thaiv corrosion zoo heev (1, 000+ teev ntsev tsuag), tab sisDX51D + AZ yog qhov nyiam rau cov dej hiav txwv xa tawmRaws li EN 10346 kev lees paub thoob ntiaj teb. Rau Suav ntug hiav txwv dej hauv tsev, DC51D + AZ yog qhov kev xaiv txhim khu kev qha.
Q5: Dab tsi substrate GNEE STEEL siv rau DX51D + AZ?
A5: GNEE STEEL muabOb txoj kev xaiv substrate rau DX51D + AZ: kub- dov DD11 (tus nqi- zoo) thiab txias- dov DC01 (kev ua tau zoo sib xws), sib piv DC51D + AZ lub substrate zoo rau siab - thov kev thov.
Q6: Puas yog ob qib muaj tib txoj kev kho mob saum npoo?
A6: Yog. GNEE STEEL muab cov kev kho saum npoo zoo ib yam rau ob qib:chromium-dawb passivation (eco-tus phooj ywg), ntiv tes-resistant (AFP), oiled, los yog unoiled, ntsib ntau yam kev xav tau ntawm daim ntawv thov.
Q7: Lub sij hawm xa tuaj rau GNEE STEEL galvalume steel yog dab tsi?
A7: Lub sijhawm khoom xa tuaj yog15-20 hnubtom qab kev txiav txim pom zoo, nrog ceev ceev 7-10 hnub xa khoom muaj rau kev txiav txim ceev. Peb muab tag nrho MTC thiab thib peb-cov ntaub ntawv xeem tog neeg (SGS/BV) raws li kev thov.
Q8: Yuav ua li cas paub qhov txawv ntawm DX51D + AZ thiab DC51D + AZ hauv cov khoom tiag?
A8: Kos qhovzeb daim ntawv pov thawj thiab cov khoom cim: DX51D + AZ yog cim nrog EN 10346, thaum DC51D + AZ siv Q / BQB 425. GNEE STEEL cov ntawv sau tag nrho cov khoom uas muaj qib meej, tus qauv, hom substrate, thiab txheej hnyav rau kev txheeb xyuas yooj yim.