DC06 vs 08AL: Teb chaws Europe vs European Ntxiv- Sib sib zog nqus Drawing Solutions rau Automotive Manufacturing

Nov 27, 2025

Khoom Description

 

DC06 txias dov hlau yog dab tsi?

DC06 yog cov teb chaws Europe sab saum toj -tier txias dov hlau rau ntxiv - daim ntawv thov sib sib zog nqus. Nyob rau hauv Suav lag luam, nws cov counterpart ze tshaj yog08 AL, kuj tseem siv rau kev tsheb loj thiab khoom vaj huam sib luag tsim.

 

Specifications Table rau DC06 txias dov hlau

Zoo Txuj Khoom No.
dc06 ua TS EN 10130 1.0873
DC 06+ZE TS EN 10152 1.0873

 

DIN EN Txuj Kev ntsuas kev taw qhia Yield Point Re
(MPa)
Tensil zog
Rm(MPa)
Elongation
A80(hauv%)
r90 n90
10130 Q Tsawg dua los yog sib npaug li 170 270 – 330 Ntau dua lossis sib npaug li 41 Ntau tshaj los yog sib npaug rau 2,1 Ntau dua lossis sib npaug rau 0,220
10152 Q Tsawg dua los yog sib npaug li 180 270 – 350 Ntau dua lossis sib npaug li 41 Ntau tshaj los yog sib npaug rau 2,1 Ntau dua lossis sib npaug rau 0,210

 

C
%
Mn
%
P
%
S
%
Ti
%
Tsawg dua lossis sib npaug li 0,02 Tsawg dua los yog sib npaug li 0,25 Tsawg dua lossis sib npaug li 0,020 Tsawg dua lossis sib npaug li 0,020 0,3

 

DC06 vs 08AL - Cov lus ua haujlwm

Parameter 08 AL dc06 ua
Kev ua tau zoo Siab heev Qib siab kawg
Txheej Smoothness Siab Siab heev
Nqi Advantage Kev lag luam ntau dua Nruab nrab
Export Kev Lag Luam Txais txwv Ntiaj teb no OEM- pom zoo

 

Cold Rolled Steel Qib Hierarchy

Qib Kev tsim qib
dc01 ua Txuj
dc03 ua Txhim kho
dc04 ua Siab
dc05 ua Siab heev
dc06 ua Sab saum toj / Ntxiv - kos duab tob

 

Vim li cas Automotive OEMs nyiam DC06

Txawm hais tias ob qho tib si DC06 thiab 08AL xa cov kev ua haujlwm siab, cov neeg tsim hluav taws xob thoob ntiaj teb nyiam DC06 vim:
🔹 Ntau- ntawv pov thawj
🔹 Qhov chaw qis qis
🔹 Ntau dua repeatability hauv pawg stamping
🔹 Muaj cov saw hlau muaj zog los ntawm cov zeb thiab cov xa tawm

DC06 ua kom lub vaj huam sib luag ruaj khov zoo thaum txo cov pwm hnav, lub sijhawm siv hluav taws xob thiab cov khoom seem- tseem ceeb rau kev tsim tsheb ntshiv.

 

GNEE STEELkuj ua tau lwm yam txias- dov steel qib. Yog tias koj muaj kev xav tau rau txias- dov steel phaj, txias- dov steel coils, galvanized steel daim hlau, lossis galvanized steel coils, thov hu rau peb. Peb yuav muab cov lus qhia tseeb rau koj!
 