DC01 Cold Rolled Steel Chev - Optimized Rau Cov Neeg Esxias Qab Teb Muaj Kev Lag Luam

Mar 12, 2026

txias dov steel kauj

 

DC01 txias dov steel kauj yog cov khoom siv dav dav dav dav hlau txias txias rau cov tuam txhab lag luam hauv Nyab Laj, Thaib, thiab Indonesia. Nws muaj cov qauv zoo heev, kev ua haujlwm ruaj khov, thiab kev siv dav dav. GNEE STEEL muab siab - zoo DC01 txias dov steel kauj nrog daim ntawv pov thawj puv, qhov ntau thiab tsawg, thiab xa khoom zoo los txhawb koj cov khoom.

 

DC01 yog tsim raws li EN 10130 tus qauv, haum rau khoov, stamping, vuam, thiab kho qhov chaw. Nws yog dav siv hauv cov khoom siv hluav taws xob, cov khoom siv tsheb, cov rooj tog hlau, cov khoom siv, thiab cov tshuab dav dav. Peb DC01 pab cov tuam ntxhab txhim kho cov khoom zoo thiab txo cov nqi.

 

Cold-rolled steel coil

Txias-rolled steel coil ntau lawm cog

 

Tshuaj muaj pes tsawg leeg ntawm DC01

 

Element C Mn P S Al
Feem pua Tsawg dua lossis sib npaug li 0.10% Tsawg dua los yog sib npaug li 0.50% Tsawg dua lossis sib npaug li 0.035% Tsawg dua lossis sib npaug li 0.025% Ntau dua lossis sib npaug li 0.020%

Tsawg carbon thiab impurity cov ntsiab lus kom zoo ductility thiab nto zoo.

 

Mechanical Properties ntawm DC01

 

Qib Tensile zog (MPa) Yield zog (MPa) Elongation (%)
dc01 ua 270 – 410 130 – 260 Ntau dua lossis sib npaug li 28

Cov txiaj ntsig no ua kom muaj kev ruaj khov thaum lub sijhawm ua haujlwm thiab txo qis kev pheej hmoo tsis ua haujlwm.

 

Specifications

 

Khoom npe

DC01 Cold Rolled Steel Chev

Txheej txheem ntau lawm

Kub Rolling, Txias Rolling

Khoom siv Standards

AISI, ASTM, ASME, DIN, BS, EN, ISO, JIS, GOST, SAE, thiab lwm yam.

Dav

45mm-2200mm

Ntev

Custom Size

Thickness

Kub Rolling: 2.75mm-100mm
Txias Rolling: 0.2mm-3mm

Kev Xa Khoom

Rolling, Annealing, Quenching, Tempered lossis Standard

Txheej txheem nto

Ordinary, Hlau Drawing, Laminated Zaj duab xis

 

Nug rau Sample & Quote

 

Specification Range

 

Thickness: 0.2-3.0 hli

Dav: 600-1600 mm

ID: 508mm / 610mm

Luj: 3-18 tons

Ntug: Mill edge / Slit edge

Nto: Bright, oiled

Kev cai slitting thiab txiav yog muaj.

 

Core Zoo

 

  • Precision Dimensional kam rau uaHigh -precision dov kom nruj tuab thiab dav kam rau ua, txhim kho cov khoom sib xws.
  • Zoo heev FormabilityZoo elongation thiab nruab nrab yield zog txo kev tawg ntawm dabtsi yog khoov thiab stamping.
  • Haum rau Kev Kho HniavLub ntsej muag huv si txhawb kev pleev xim, electroplating, thiab galvanizing nrog siab tiav.
  • Kev xa khoom ruaj khov & Kev xa khoom saiCov khoom lag luam loj thiab cov khoom lag luam paub tab kom paub meej txog - lub sijhawm xa tuaj rau Asia.

 

Daim ntawv thov kev lag luam hauv Nyab Laj, Thaib & Indonesia

 

  • Hluav taws xob & Electronics: Control lub thawv, lub cev muaj zog plhaub, panels
  • Cov Khoom Siv Hauv Tsev: Cua txias, tub yees, tshuab ntxhua khaub ncaws
  • Automotive & Maus taus: Brackets, npog, tsis yog - cov yam ntxwv
  • Hlau rooj tog:Txee, txee, ncej
  • Kev tsim kho:Cov yeeb nkab, profile, cov khoom siv kho kom zoo nkauj

 

Quality Assurance

 

ISO 9001 tau ntawv pov thawj

Daim ntawv soj ntsuam tag nrho

Mill daim ntawv pov thawj muaj

Thib peb- tog neeg soj ntsuam tau txais

 

Cold Rolled Steel Coil

Txias Rolling Laboratory

Kev Pabcuam

 

Kev cob qhia kev xaiv cov khoom siv

Customized ua

Cov lus ceev ceev

ruaj khov tom qab - kev muag khoom

Logistics taug qab

 

DC01 yog tus nqi- siv tau zoo thiab siv tau dav, sib piv cov kev xav tau ntawm kev tsim khoom hauv Nyab Laj, Thaib, thiab Indonesia. ruaj khov zoo thiab ua tau yooj yim ua rau nws irreplaceable.

 

DC01 txias dov steel kauj yog qhov tseem ceeb rau kev tsim khoom niaj hnub. GNEE STEEL muab siab - cov khoom zoo thiab cov kev pabcuam tshaj lij los pab koj ua tiav hauv kev sib tw ua lag luam Esxias sab hnub tuaj.

 

Hu rau GNEE STEEL hnub no kom tau txais koj qhov kev thov zoo tshaj plaws rau DC01 txias dov steel kauj.

 

DC01 Cold Rolled Steel Coil

Neeg tuaj xyuas

Xa kev nug

Xa kev nug