Sib piv Galvanized Steel Chev (GL) thiab Aluminium - magnesium - zinc coated steel

Oct 11, 2025

Aluminium magnesium Zinc Txheej (Almgzn):

 

Nrov cov lus qhia tshwj xeeb yog qhov tsis txaus!
Nyem kom tau txais daim ntawv tshwj xeeb!

Tuam Tshoj Aluminium No Zinc Coated Steel Chev Khoom Siv, Zoo Tshaj Plaws Corrosion (tshwj xeeb tshaj yog tsis kam rau xim liab thiab ntug kev tiv thaiv)
Qhov no yog qhov tseem ceeb tshaj plaws thiab tseem ceeb kom zoo dua ntawm txhuas magnesium zinc txheej.

Aluminium magnesium Zinc Txheej (Almgzn):

1. Kev tiv thaiv Barrier:

Aluminium (Al) cov ntaub ntawv tuab thiab ruaj khov ntawm txhuas oxide (al ₂ o3) zaj duab xis nyob rau txheej txheej ntawm cov kev sib chwv ntawm txoj kev sib chwv ntawm txoj kev tawm suab thiab sab hauv.
2. Tshuaj Tiv Thaiv Anode Anode:

Zinc (ZN) thiab magnesium (mg) muab cov tshuaj ntsuab muaj zog "kev tiv thaiv. Tshwj xeeb nrog nrog ntxiv ntawm magnesium (mg), nws cov tshuaj lom neeg yog siab dua li ntawm zinc, thiab nws tuaj yeem muab cov khoom tiv thaiv tam sim no ntxiv thiab ua kom zoo.
3. Kev kho tus kheej:

Corrosion cov khoom ntawm magnesium (xws li Magnesium hydroxide mg (Oh) yuav them rau qhov kev txiav txim siab, sau cov txheej txheem tiv thaiv corrosion, ua kom muaj kev tiv thaiv kev tiv thaiv corrosion. Qhov no yog nws cov yees duab ntug tus kheej kho lub peev xwm.
4.Rovult:

Nws corrosion resistance (tshwj xeeb yog nws tiv taus liab xeb) feem ntau yog 2-4 zaug lossis siab dua li ntawm cov ntshiab zinc Txheej ntawm qhov hnyav. Qhov no txhais tau tias nyob rau hauv tib qho kev ua kom xeb ib puag ncig corrosive, cov tais thij thoj siv tau los ua kom tau kev pab them nqi ntev ntev xws li ru tsev thiab nkhaus.

 

Aluminum Magnesium Zinc Coating (AlMgZn)

 

Galvanized steel coil (GL) vs txhuas - Magnesium - zinc coated steel

 

AlMgZn or ZM coated steel coils

 

Gnee steelTshwj xeeb hauv Muag AL MG ZN ZE coated steel daim hlau thiab muab kev ua, shearing, thiab kev pabcuam tsheb thauj mus los. Yog tias koj xav tau yuav ,. Thov xa email rau kuv:info@gneegi.com

 