Tuam Tshoj Cold Rolled Steel Sheet Phaj Strip Chev DC01 DC03 DC04 DC05 DC06

Nov 27, 2025

Txias Rolled Steel

 

DC01, DC02, DC03, DC04, DC05, DC06 yog tus qauv European txias- dov qis- carbon steels teev nyob rau hauv EN 10130 rau qhov chaw uas yuav tsum tau formability zoo heev thiab zoo ib yam nto. Rau cov txheej txheem xovxwm - cov khoom tsim, DC03–DC06 yog cov kev xaiv ntau; DC01 thiab DC02 yog qhov tsim nyog thaum lub zog siab dua me ntsis lossis kev coj ua deoxidation sib txawv tau txais. Rau cov neeg yuav khoom nrhiav kev sib tw khoom los ntawm Tuam Tshoj,

GNEE STEELmuaj lub Hoobkas- tus nqi ncaj qha, xa khoom sai, thiab cov ntaub ntawv xeem kom tau raws li EN 10130 cov cai. Thaum xaiv cov qib, ua qhov tseem ceeb ntawm lub hom phiaj tsim qhov hnyav, qhov yuav tsum tau ua tiav (A lossis B), thiab seb cov khoom siv coated (galvanized) raws li EN 10152 xav tau.

 

Cold Rolled Steel

 

Tshuaj muaj pes tsawg leeg

Qib C Mn P S Alta
DC01, SWB Tsawg dua lossis sib npaug li 0.12 Tsawg dua lossis sib npaug li 0.60 Tsawg dua lossis sib npaug li 0.045 Tsawg dua lossis sib npaug li 0.045 Ntau dua lossis sib npaug rau 0.020
DC02, SWB Tsawg dua lossis sib npaug li 0.10 Tsawg dua lossis sib npaug li 0.45 Tsawg dua lossis sib npaug li 0.035 Tsawg dua lossis sib npaug li 0.035

Ntau dua lossis sib npaug rau 0.020

DC03, SWB Tsawg dua lossis sib npaug li 0.08 Tsawg dua los yog sib npaug li 0.40 Tsawg dua lossis sib npaug li 0.030 Tsawg dua lossis sib npaug li 0.030 Ntau dua lossis sib npaug rau 0.020
DC04, SWB Tsawg dua lossis sib npaug li 0.06 Tsawg dua los yog sib npaug li 0.35 Tsawg dua lossis sib npaug li 0.025 Tsawg dua lossis sib npaug li 0.025 Ntau dua lossis sib npaug rau 0.015

 

Mechanical Properties

Qib RCL (Mpa) RM (MPa) A80mm (%) R90 N90
dc01 ua 140~280 270~410 Ntau dua lossis sib npaug li 28    
dc02 ua 140~240 270~370 Ntau dua lossis sib npaug li 34 Ntau dua lossis sib npaug rau 1.4  
dc03 ua 120~210 270~350 Ntau dua lossis sib npaug li 38 Ntau dua lossis sib npaug rau 1.8 Ntau dua lossis sib npaug rau 0.18
dc04 ua 120~180 270~330 Ntau dua lossis sib npaug li 40 Ntau dua lossis sib npaug rau 2.0 Ntau dua lossis sib npaug rau 0.20
SPCC 130~300 270~410      
SPCD 120~240 270~370   Ntau dua lossis sib npaug rau 1.3  
SPCE 120~210 270~350   Ntau dua lossis sib npaug rau 1.8 Ntau dua lossis sib npaug rau 0.18

 

Daim ntawv thov scenarios ntawm txias-qib dov

Peb lub tuam txhab tseem tuaj yeem muab cov khoom txias hauv qab no - dov steel qib:
DC01 - Tsim los rau cov txheej txheem tsim cov txheej txheem xws li khoov, embossing, hlaws thiab cov qauv kos duab.
DC03 - Npaj rau kev thov ntau daim ntawv thov, suav nrog kev kos duab sib sib zog nqus thiab ntau qhov profile.
DC04 - Haum rau cov ntawv thov uas xav tau qib siab ntawm formability.
DC05 – Qhov sib sib zog nqus- qib kos duab tsim los ua kom tau raws li qhov yuav tsum tau ua ntau yam.
DC06 - Ib qho tshwj xeeb sib sib zog nqus- qib kos duab tsim rau qhov kev xav tau siab tshaj plaws hauv kev ua kom txias.
DC07 - Ib qho kev sib sib zog nqus tob heev -qib duab kos rau kev ua haujlwm hnyav thiab nyuaj heev.

 

GNEE STEELkuj ua tau lwm yam txias- dov steel qib. Yog tias koj muaj kev xav tau rau txias- dov steel phaj, txias- dov steel coils, galvanized steel daim hlau, lossis galvanized steel coils, thov hu rau peb.Peb yuav muab cov lus qhia tseeb rau koj!
 