TS EN 10346 Qib S350GD Zinc{2}}Aluminium-Magnesium Coated (+ZM)

Magnelis® yog cov khoom lag luam tiaj tus carbon steel coated ntawm ob sab nrog zinc{0}}aluminium-magnesium alloy. Cov hlau no, muaj li ntawm 93.5% zinc, 3.5% aluminium thiab 3% magnesium, yog siv los ntawm kev siv cov txheej txheem kub dip galvanizing. Qhov zoo tshaj plaws tshuaj muaj pes tsawg leeg tau raug xaiv los muab cov txiaj ntsig zoo tshaj plaws ntawm kev tiv thaiv corrosion.

Khoom Taw qhia

Khoom Taw qhia

Gnee Steel (Tianjin) Co., Ltd. yog ib qho ntawm feem txhim khu kev qha manufacturers thiab lwm tus neeg ntawm en 10346 qib s350gd zinc-aluminium-magnesium coated (+zm) nyob rau hauv Suav teb. Txais tos rau kev lag luam wholesale customized en 10346 qib s350gd zinc{10}}aluminium-magnesium coated (+zm) ntawm tus nqi qis los ntawm peb lub hoobkas. Yog tias koj muaj lus nug txog cov qauv dawb thiab cov khoom pheej yig, thov koj xav email rau peb.

 

EN 10346 Grade S350GD Zinc-aluminium-magnesium Coated (+ZM)

EN 10346 Grade S350GD Zinc-aluminium-magnesium
Cov khoom

Dimension

Khoom Tus nqi

Qhov ntev

Thov koj xav mus xyuas daim duab ntawm sab xis ntawm nplooj ntawv cov ntaub ntawv kom paub meej ntxiv.

Neeg kho tshuab

Khoom Tus nqi Saib

Elongation

 

12 %

 

min.|rau thickness 0.45-0.5 mm|A80

 

14 %

 

min.|rau thickness 0.5-0.7 mm|A80

 

16 %

 

min.|rau thickness 0.7-6 mm|A80

Tensile zog

 

420 MPa rau

 

min.|rau thickness 0.45-6 mm

Yield zog

 

350 MPa

 

min.|rau thickness 0.45-6 mm

Cov khoom siv tshuaj

Khoom Tus nqi Saib

Cov pa roj carbon

0.2 %

 

max.

Manganese

1.7 %

 

max.

Phosphorus

0.1 %

 

max.

Silicon

0.6 %

 

max.

Sulfur

0.045 %

 

max.

Cov cuab yeej technology

Khoom    
Cov chaw thov

 

Magnelis® tuaj yeem siv rau hauv ntau daim ntawv thov kev lag luam, xws li:

Hnub ci zog tiam: cov qauv rau photovoltaic thiab thermal solar nroj tsuag

Kev tsim kho: cov qauv lossis tsis yog- cov qauv txheej txheem, vov tsev & cladding, decking, cable tais, nthuav hlau, gratings, composite flooring, qhob pwm

Txoj kev thiab railway infrastructure: kev nyab xeeb teeb meem, cov khoom tiv thaiv, suab rwb thaiv tsev phab ntsa panels, phab ntsa muab kev tiv thaiv los ntawm lawg

Kev ua liaj ua teb thiab ua liaj ua teb: barns, tsev cog khoom vaj tse, khoom siv ua liaj ua teb

Tubular daim ntaub ntawv: structural raj rau scaffolding, txoj kev teeb liab, ncej

Cov ntawv pov thawj

 

Magnelis® tau pom zoo siv hauv Kev Tsim Kho Kev Tsim Kho los ntawm ntau lub teb chaws:

Lub teb chaws Yelemees: DIBt Z-30.11-51 rau Magnelis®

Fabkis: ETPM rau Magnelis® los ntawm CSTB

Sweden: Technical Approval No. SC0559-13 rau Magnelis®

 

Tshuaj muaj pes tsawg leeg

Yog tias, los ntawm kev pom zoo thaum lub sijhawm nug thiab kev txiav txim, lwm yam tshuaj lom neeg ntxiv, lawv yuav tsum tau hais rau ntawm daim ntawv tshuaj ntsuam xyuas uas yuav xav tau kev hloov pauv.

 

Txheej

 

Magnelis® Txheej hnyav - ob sab (g / m²) Txheej thickness (µm ib sab) *
ZM 70 70 5
ZWM 90 90 7
ZWM 120 120 10
ZWM 175 175 14
ZM 200 200 16
ZWM 250 250 20
ZWM 310 310 25
ZWM 430 430 35
* Cov txheej hnyav ntawm lub rooj no tau suav nrog qhov ceev ntawm Magnelis®.

 

Qhov ceev ntawm Magnelis® txheej yog 6.2 g / cm3, vim nws cov tshuaj muaj pes tsawg leeg.

 

Lwm yam

 

Cia

Magnelis® yog muab passivated thiab / los yog oiled los txwv ib ntus kev pheej hmoo ntawm xeb dawb tsim. Thaum thauj thiab khaws cia, tag nrho cov kev ceev faj tsim nyog yuav tsum tau ua kom cov khoom kom qhuav thiab tiv thaiv kev tsim ntawm condensation.

 

Cov txheej txheem ua

 

Cov txheej txheem tsim tam sim no siv rau cov hlau galvanized kuj haum rau Magnelis®. Magnelis® coj zoo heev thaum ua haujlwm profile. Cov txheej tuab yuav tsum tau sib haum nrog ob qho tib si qib siab ntawm kev tiv thaiv corrosion thiab cov kev cai ntawm kev tsim cov txheej txheem envisaged. Qhov tsawg kawg yog dabtsi yog khoov vojvoog ntawm 2x daim ntawv thickness yog pom zoo.

 

Vuam

Nyob rau hauv qhov chaw vuam, qhov vuam tam sim no yuav tsum raug tswj kom haum thiab hloov kho tsis tu ncua. Electrode lub neej tuaj yeem txuas ntxiv los ntawm kev nce qib ntawm cov vuam tam sim no thiab ua ntu zus (machining) cov electrodes. Cov txheej thickness yuav tsum tau sib xws nrog ob qho tib si qib siab ntawm kev tiv thaiv corrosion thiab cov kev xav tau ntawm cov txheej txheem vuam envisaged. Magnelis® tuaj yeem ua arc welded, laser welded, brazed lossis siab zaus induction welded, ua tib zoo ceev faj ib yam li cov hlau galvanized. Rau siv nyob rau hauv sab nraum zoov daim ntaub ntawv ib tug reprotection ntawm weld seams los ntawm arc vuam thiab siab zaus induction vuam yog pom zoo.