Gnee Steel (Tianjin) Co., Ltd. yog ib qho ntawm feem txhim khu kev qha manufacturers thiab lwm tus neeg ntawm sefc440 electrolytic zinc-coated steel nyob rau hauv Suav teb. Txais tos rau kev lag luam wholesale customized sefc440 electrolytic zinc-coated steel ntawm tus nqi qis los ntawm peb lub hoobkas. Yog tias koj muaj lus nug txog cov qauv dawb thiab cov khoom pheej yig, thov koj xav email rau peb.
Khoom: Electrolytic zinc-coated steel ntawv thiab coils
Qib: SEFC440
SEFC440 steel zoo: Kev tsim zoo
SEFC440 steel cais cov cim ntawm lub hauv paus hlau hauv JIS: SPFC440
SEFC440 steel Chev / sawb / ntawv kho qhov chaw:
C (Chromate kho), P (phosphate kho), M (tsis kho), O (oiled), X (unoiled)
SEFC440 steel Chev / sawb / daim ntawv nto structural: N5 (Ntiv tes tsis kam)
SEFC440 steel Chev / sawb / ntawv txheej loj: ES, EB, E8, E16, E24, E32, E40
JIS G 3313 SEFC440 steel siv nominal thickness: 0.6mm los yog tshaj li thiab incl . 2.3mm
SEFC440 steel chemical muaj pes tsawg leeg % : Xa mus rau cov tshuaj muaj pes tsawg leeg ntawm SPFC440
SEFC440 steel Mechanical zog
| Qib |
Yield zog MPa |
Tensile zog MPa |
Elongation % min |
|||||
|
0.4- Tsawg dua los yog sib npaug rau 0.6mm |
0.6- Tsawg dua lossis sib npaug li 1.0mm |
1.0- Tsawg dua lossis sib npaug li 1.6mm |
1.6- Tsawg dua lossis sib npaug li 2.3mm |
2.3- Tsawg dua los yog sib npaug li 2.5mm |
2.5 los yog ntau tshaj |
|||
|
SIB 440 |
265 feeb |
440 min |
- |
26 |
27 |
27 |
- |
- |
GNEE STEEL muaj ntau tshaj 2000 tons SEFC440 steel Tshuag qhov chaw txhua lub hlis. Peb tuaj yeem ua tau raws li peb cov neeg siv khoom feem ntau ntawm qhov ntau thiab kev thov. Raws li cov khoom lag luam no, peb qhov kev lag luam zoo tshaj plaws kis mus rau cov txheej txheem steel xws li: txiav (ntawm qhov dav thiab ntev), kos duab, rov ntim dua, thiab lwm yam.

Cim npe nrov: sefc440 electrolytic zinc-coated steel, Tuam Tshoj sefc440 electrolytic zinc-coated steel manufacturers, lwm tus neeg, Hoobkas